The consumables are arranged according to the yield strength (Rₚ₀.₂) for which they are classified. In reality, a given consumable normally has a higher yield strength than its standard designation. The mechanical properties of a given consumable can be obtained from its manufacturer.
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
AWS Class
400 (58)
E7016-X*, E7018-X*
470 (68)
E8016-X*, E8018-X*
540 (78)
E9018-X*
610 (97)
E10018-X*
680 (100)
E11018-X*
745 (108)
E12018-X*
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
ELGA
400 (58)
P48S, P51
470 (68)
P48K, P65MR
540 (78)
610 (97)
680 (100)
P110MR 
745 (108)
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
ESAB
400 (58)
OK 48.00, OK 48.50
470 (68)
OK 73.68, OK 73.15
540 (78)
OK 74.78
610 (97)
OK 74.86 Tensitrode
680 (100)
OK 75.75, Filarc 118
745 (108)
OK 75.78
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
LINCOLN ELECTRONIC
400 (58)
Basic 7018, Baso 100
470 (68)
Conarc 74
540 (78)
Conarc 60G, Conarc 70G
610 (97)
680 (100)
Conarc 80
745 (108)
Conarc 85
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
BÖHLER
400 (58)
Fox ev 50, AWS E7018-1
470 (68)
Fox ev 60, Fox Fox 2.5Ni
540 (78)
Fox ev 70
610 (97)
680 (100)
Fox EV 85, Fox alform 700
745 (108)
Consumable manufacturer/ Min yield strength MPa (ksi)
Consumable manufacturer/ Min yield strength MPa (ksi)
OERLIKON
400 (58)
Carbofil 1, Carbofil 1 Gold 
470 (68)
Tenacito 70
540 (78)
Tenacito 65R
610 (97)
Tenacito 75
680 (100)
Tenacito 80
745 (108)
Tenacito 100

* X can stand for one or several code characters

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026