How to bend > How to press brake > How to set up the work piece

Die width

When plate thickness increases, the die width often needs to be increased as well.

However, how die width is measured can vary between different manufacturers and companies.

U-Die with wall-to-wall die width definition. 

V-Die with roll-to-roll die width definition (e.g. Trumpf style die). 

V-Die with edge-to-edge die width definition (e.g. WILA style die). 

As shown in the illustrations above, some dies are equipped with die rollers to reduce friction during bending.

Even if the die does not have visible rollers, it still features a small radius at the bottom to facilitate material flow and minimize friction.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026