Bucket design > Carbon footprint of buckets

How to save carbon emissions

A bucket’s carbon footprint can be reduced in several ways.

Less steel produced


With wear-resistant, high-strength steel, less steel is needed, resulting in a lower embedded carbon footprint from the steel production. In addition, a steel with lower or zero carbon emissions cut the carbon emission further. SSAB has already one of the world’s most efficient steelmakers, and products with zero-emission steels.

Longer service life


Wear-resistant steel combined with good structural design, make the bucket to last longer. If the lifetime is doubled, embedded carbon emissions over the product lifecycle is only half.

Lower weight


With lower weight, the wheel loader or excavator will need less fuel for the same work. Every 1000 liters of diesel not used saves 3 tonnes of CO2.
Finally, a bucket design with higher productivity and a longer lifetime results in a lower carbon footprint to move the same amount of bulk material.

Higher capacity


When a bucket is lighter, its payload can be increased, resulting in fewer swings for the same material moved.  Every present of increased load capacity results in the same percentage of fuel and carbon emission savings.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026