Deutsche Bahn renews and expands approval for SSAB steel for bridge applications

SSAB Weathering, Structure and bridges
May 17, 2022 8:00 CEST
Weathering and high-strength thermomechanically rolled steel plates and hot rolled strip products from SSAB’s Raahe mill are now approved by Deutsche Bahn for use in bridges.

bridges and structures

Deutsche Bahn, the railway regulator whose DBS 918002-2 standard is used for building both train and road bridges in Germany, has qualified SSAB’s Raahe, Finland mill for a wide range of hot-rolled steel heavy plates and wide strips in accordance with DIN EN 10025-2, -3, -4 and -5.

SSAB Weathering steels can be used on a variety of bridge structures, including I-beams/girders, cross members, trapezoidal sections, and piers. SSAB Weathering steel eliminates the need for painting and anti-corrosion treatments, significantly reducing CO2 emissions generated by coating maintenance.

Previously, SSAB’s Raahe mill was certified by Deutsche Bahn for steel plate and strip products according to DIN EN 10025-2. With the new DB approval, bridge and infrastructure engineers will now have additional steel options for their designs.

For more information on SSAB Weathering steel for bridges, visit SSAB Weathering - Structure and bridges. 

For further information, please contact:
Lutz Felder, Marketing Manager
[email protected], phone +49 151 16750234

Manufacturer related product qualification

Related articles

Other newsSSAB Weathering steel defies marine conditions on the Huikku Bridge in Hailuoto
SSAB Weathering
Other newsWorld’s first robotically welded automated bridge: The Ya Bridge, Norway
SSAB Weathering
Product press releasesSSAB – The only approved COR-TEN® manufacturer in Europe
ASTM, COR-TEN, SSAB Weathering