R/S Godwin sets new standard in dump bodies

5 min read

Country

United States

Company

The Godwin Group: R/S Godwin

Industry

Trailers and body builders

Brand program

Hardox® In My Body

Going from good to great, The Godwin Group upgrades its full product line at R/S Godwin to Hardox® 500 Tuf to deliver the next-generation of wear-resistant steel to customers right from the start.

“At the end of the day, a dump body is a dump body,” says Pat Godwin, President of The Godwin Group located in Dunn, North Carolina, U.S. 

“What makes it different is the durability, and with trucks becoming harder to get and at higher prices, it is more important than ever that we continue our practice of offering high value equipment that is going to last." That’s why the company now builds its entire heavy duty dump body portfolio using only Hardox® 500 Tuf, the next-generation of wear-resistant steel.

Watch the full story – a comittment to build the best

Watch the full story in the video

Hear why this leading family-owned truck equipment manufacturer upgraded its entire heavy-duty dump body portfolio to be built using Hardox® 500 Tuf as its standard steel specification.

American-made dump bodies for the long haul

Growing from a one-man, backyard shop in 1966 to a multi-brand operation with five locations across three states, the company’s founder, Pat Godwin Senior, established a simple mantra solidifying six decades of success – Build the best. 

To achieve that in the early days, the design philosophy called for thicker steel and stiffing joints to produce a heavier, sturdier dump body option with reinforced floors. While this method produced a durable body, its added significant weight to the overall truck’s design and took money out of the operator’s pocket. 

“They were having to haul less and less,” Pat explains. “You know, whether it’s one extra load or two extra loads, I mean, it all adds up at the end of the year. Now, with the Hardox® 500 Tuf, we can build bodies lighter and stronger than they have ever been before. Not only is the operator getting a bed that’s three times stronger than it used to be, it's actually twelve-hundred pounds lighter. That means every single load he hauls, he can haul twelve-hundred pounds more.”  

That’s a substantial improvement for dump truck owners and operators like Thomas Hamman with Dynamic Trucking. “In our business, we are paid based on weight,” Hamman explains. “So, if we’re able to have all the durability from the steel, while at the same time being able to load more product into our truck, I mean, it’s a win-win for us.” 

Show me next-gen hard & tough

Not all high-strength steel is created equal

According to Patrick Godwin, the family-owned company’s Marketing Director, ”What a customer should be asking, when they're looking for a dump body is, what's going into it, and how is it built?”

“All steel is not created equal,” says Shawn Auxier, General Manager. “Hardox® wear plate, to me, is the best material out there because it’s so significantly better than other steels on the market. Hardox® material is a much stronger application.” 

Manufacturers using Hardox® 500 Tuf see longer wear life oftentimes up to 40% longer and are changing the game in their industries. 

According to Johnny Stockman at TLG Peterbilt, ”Godwin just took over the market because they outperformed everybody. The body, once it’s put together, you never hear from it again.

I want to improve my product design - contact me

Making friends in the workshop

The advantages of Hardox® wear plate don’t stop with long wear life and tough performance in the field. To ensure predictable fabrication in the workshop, Hardox® 500 Tuf is a clean steel with extremely consistent, guaranteed properties for flatness, thickness and bending performance. 

Upgrading to Hardox® 500 Tuf is a smooth process. It can be welded using any conventional technique, with no or low pre-heating requirements up to 38.1 mm (1.5 in.). The same applies for cutting, bending, and machining.

“In your mind you kind of think, “oh it’s stronger, it’s going to be harder to work with, but that wasn’t the case,” says Chris Saylor, Purchasing Manager at The Godwin Group. “Hardox® 500 Tuf is easy to cut, easy to bed, easy to weld. All the Hardox® wear steel we buy is made here in the United States.” 

I want to see the guarantees

Quality at the next level is certified Hardox® In My Body

The Hardox® In My Body sign on an Original Equipment Manufacturer’s product is a confirmation of quality, performance, reliability and productivity for customers everywhere. Only equipment that has been certified to meet the strictest standards of quality in design and fabrication may display the Hardox® In My Body sign. The sign is an acknowledgement of a members’ dedication to providing high-quality, high-performing and cost-efficient products.

“Hardox® In My Body is a serious statement,” says Pat. “By joining forces with SSAB and having Hardox® wear plate in our body, it means a lot to us because it enables us to not be complacent, and it allows us to be aggressive in our market.

Level up! What is Hardox® In My Body?

Innovation through close collaboration

Thanks to its century-long expertise in steelmaking, SSAB introduced Hardox® wear plate in 1974, setting at new industry standard for hard and tough wear-resistant steel. Since then, SSAB continues to transform the steel industry driven by close relationships with customers.

“SSAB has been an amazing partner to work with,” says Patrick. “We truly feel to our heart and core that our product offerings are the best on the market. And that’s one of the things that we’re striving to do within all of The Godwin Group of companies, it’s to be innovators in our industry. We feel like SSAB has been an integral part of that.

Ready to step up your steel?

Join companies like The Godwin Group and step up from average abrasion-resistant (AR) steel to Hardox® wear plate - the world’s only wear-resistant steel for extreme applications.

I’m ready to step up my steel

Stay up to date on the benefits of Hardox® wear steel

Hardox Product Overview

Check out the Hardox® range

How to increase load, save on maintenance and extend service life

See how
Download App

Find the right type of wear plate

Try our Hardox® WearCalc application and calculate how long the life of your products will increase and the payload will increase with a replacement for a Hardox® wear plate.

Download the WearCalc application
Hardox in my body

Guarantee of a good choice

The Hardox® In My Body brand on your devices is a guarantee of quality, performance and reliability.

Introduction to the Hardox® In My Body brand
Copyright 2026