Excavator bucket manufacturer ChangWoon goes for 100% Hardox® 500 Tuf to save weight and extend service life

3 min read

A caterpillar truck with bucket made in Hardox® 500 Tuf steel.

Country

Korea, Republic of

Company

ChangWoon Industry

Industry

Construction, demolition & road building machinery

Brand program

Hardox® In My Body

Think it’s impossible to reduce a bucket’s steel gauge thickness yet boost service life? Think again. ChangWoon switched from S45C (S355, G50) steel to Hardox® 500 Tuf, in some cases extending wear life up to 400%.

A first for excavator bucket manufacturers in South Korea – 100% Hardox® 500 Tuf

ChangWoon has been quick to adapt its own patented bucket design to the performance potential that comes with Hardox® 500 Tuf, using only this steel for both wear resistance and structural strength. The steel’s combination of high hardness and high toughness makes it a perfect material for light, strong and durable excavator buckets. Naturally, having one steel for different parts has both logistic and processing benefits. It improves yield and speeds up production when bending and welding the steel.

Get free technical advice from SSAB’s experts
The Hardox® 500 Tuf name printed all over the inside of a strong and tough steel digging bucket made by excavator bucket manufacturer ChangWoon.

Why Hardox® 500 Tuf beats mild steel in buckets and shovels

Many of ChangWoon’s customers work with hard, abrasive materials. And the harder the material, the more important it is to carefully select the bucket’s steel. If a bucket’s structure is made of relatively mild steel like A36, grade 50, A514 or S355 steel and exposed to highly abrasive materials, its service life will be cut short and costs for repair and downtime will be high.

In traditional buckets, the steel has to be beefed up with a so-called wear package for protection and longer service life. But this kind of bucket isn’t optimized for its task. It has a lot of deadweight due to the combination of a less wear-resistant steel and additional wear parts.

With Hardox® 500 Tuf, excavator bucket manufacturers can build buckets that are both stronger and lighter than traditional buckets. This is because the steel is hard yet tough enough to function as a structural steel. ChangWoon reduced the steel thickness by 2 mm (0.079”) while maintaining or even increasing the bucket’s wear life, in some cases by as much as 400%. They could also save 17% weight or 90 kg (198 lbs.) in a 0.6 m3 (0.785 cu. yd.) bucket.

Download the Hardox® 500 Tuf spec sheet
A tooth bucket with plates made of Hardox® 500 Tuf.

First Hardox® In My Body bucket manufacturer in South Korea

Being a member of the Hardox® In My Body brand program is a proof of ChangWoon’s dedication to continuous development and quality. Its buckets are designed and manufactured according to the program’s strict specifications, using genuine Hardox® wear plate.

“Hardox® 500 Tuf and Hardox® 500 have excellent weldability and formability, which helps to bring higher performance and more sustainable quality,” says ChangWoon’s president Mr. Kang-Jun Lee. The company is certain that the membership supports its strategy to reach a leading position on the market.

Level up with Hardox® In My Body
Digging bucket made in strong and super tough Hardox® 500 Tuf steel.

ChangWoon on the road to expansion

ChangWoon has a solid reputation in the South Korean construction business. The company started in 2013 as a manufacturer of structural bridge components. In 2018 ChangWoon introduced its own line of excavator buckets made in Hardox® 500 and Hardox® 500 Tuf. The buckets have gained praise from customers in South Korea and abroad.

ChangWoon works closely with its customers to collect feedback from field operations. This drives the development process forward to optimize the performance of Hardox® wear steel in a bucket’s different parts.

Watch a complete bucket build in 100% Hardox® 500 Tuf!

Stay updated on Hardox® wear plate

Hard and tough Hardox® 500 Tuf steel in a wheel loader bucket against a dramatic gray sky.

All about Hardox® 500 Tuf in buckets

How to load more, save on maintenance and extend service life.

Here’s how
A mobile phone showing the WearCalc app

Hardox® WearCalc

The Hardox WearCalc software and mobile app make tough decision about choosing the right wear plate easy.

Try out the mobile app
A  Hardox® In My Body sticker.

Confirmation of a good choice

The Hardox® In My Body sign on your equipment is a confirmation of quality, performance and reliability.