How to weld > Welding defects and discontinuities

Lack of fusion

Read about possible causes and suitable actions to avoid them

Cause

  • Travel speed too low (weld metal starts to flow in front of the arc)
  • Travel speed too high
  • Arc voltage too low
  • Too long “stick out” distance
  • Contact tip worn out
  • Insufficient inter-run cleaning
  • Welding in inclining position (downhill)

Remedial actions

  • Increase the travel speed
  • Decrease the travel speed
  • Increase the arc voltage
  • Decrease the stick out distance
  • Replace the contact tip
  • Remove the surface slag prior to next run
  • Adjust the travel speed in relation to the position

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026