How to weld > Shielding gas

MAG welding

MAG welding is performed with different kinds of consumables including solid wires, flux cored wires and metal cored wires.

A typical shielding gas for MAG welding with these types of consumables is a mixture of argon (Ar) and carbon dioxide (CO2). Another alternative is a shielding gas consisting of 100% CO2, which can be an alternative in certain situations for MAG welding with flux cored wires.

The proportions of argon and carbon dioxide in Ar/CO2 mixtures are related to the type of arc that is applied. Some mixtures are optimized for welding with a specific arc. Others can attain favorable results when welding with more than one arc type.

The three principal arc types that are feasible during MAG welding are short arc, spray arc and pulsed arc. Solid wires, flux cored wires and metal cored wires are feasible for these three kinds of arcs.

Category and tags

How to weldShielding gas

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Related knowledge base articles

Contact technical support

Read more

Contact your local SSAB steel sales team

Read more

SSAB Locations

Read more