Toolox® prehardened steel stands up to wear and tear

Making a hard steel is easy, if you’re only looking for hardness. The tricky part is to make a steel that is both hard and tough. A steel such as Toolox®. With hardness that gives a long lifetime even with highly abrasive applications, and toughness that enables it to withstand cracks and fatigue.

Hardness and toughness

Toolox® steel is hard to the core

All Toolox® steel grades have the same hardness all the way through. You can machine Toolox® plates and round bars to any complex shape, knowing that all surfaces are equally hard.

Toolox® steel has a fine grained tempered martensitic crystalline structure, a result of quenching at a high cooling rate. The fine grain size gives high toughness.

Impact toughness, Charpy-V (J) at 20°C

The table shows the toughness of Toolox® 44 compared to some standard steels that are heat treated to 45-55 HRC. Toughness values for Toolox® at -20°C are stated in the productcertificates.

Grade
Hardness
(HB)
Yield strength
(MPa)
Tensile strength
(MPa)
Elongation
A5 (%)
Toughness at
+20°C (J)
Toolox® 33275-32585098014100
Toolox® 44410-475130014501330

 

Toolox® 33 has a nominal hardness of 300 HBW. Toolox® 44 has a nominal hardness of 45 HRC, making it the world’s hardest fully prehardened tool steel. Datasheets for all Toolox® grades are available here.

"We switched from 1.2379 steel with 56 HRC to Toolox® 44. Instead of cracking after 5,000 pieces the work piece in Toolox® 44 shows no wear after more than 40,000 pieces."
ULUS METAL, ISTANBUL
""

Read all about why Toolox® steel outperforms on every challenge

Get the full story of Toolox® engineering and tool steel from SSAB.

Download PDF
""

Read all about welding and cutting recommendations for Toolox® steel

Toolox® is easy to weld and easy to cut. In the brochure you’ll find the best practises.

Download PDF
""

Read all about machining of Toolox® steel

Toolox® is a prehardened steel with high machinability for making finished parts without time-consuming and costly heat treatment

Download PDF