Fallstudie
Smart scrap grabs grab more market share with Hardox® steel
24. September 2021 6 Min. gelesen

Fallbeispiel
After becoming a certified member of the Hardox® In My Body program, JK Technology from South Korea has seen its sales soar. Their “smart” scrap grab in particular has become its most popular product and successfully competes with other products made in lower-carbon cast steel.
JK is a leading Korean manufacturer of heavy equipment attachments for scrap and demolition, construction and forestry applications. They manufacture attachments such as quick couplers, scrap grabs, compactors, stone grapples, lifting forks, rippers and more.
With roughly 25 employees, JK is a small company with big dreams – and a growing market share both domestically and abroad. The company has a global network in the United States, Australia, New Zealand and Singapore. It currently exports 15% of its production and is on track to expand its global footprint.