Milling

Milling is a machining process where a rotary cutting tool removes material from the workpiece. Milling is normally used to machine contours to flat surfaces but also produce irregular shapes and surfaces. and can be used to drill, bore, cut gears and produce slots. There are several different types of milling machines where the vertical milling machine is the most common in workshops. Today’s new milling machines are CNC controlled, allowing for better precision and repeatability compared with manual milling.

 

Get in touch

If you have any questions or need additional information or price quote, feel free to
contact us. Our dedicated team is here for you.

CONTACT

Icon method

Method

The cutting tool, with special tool-steel and sharp vertical or fluted teeth, is secured into the milling head and rotates at very high speed and moved perpendicular or parallel to its axis. Cutting tools vary in shape and sizes and chosen based on its purpose, e.g. end mill, side-and-face cutter and gear cutter.

For a good end result, the choice of cutter and parameters such as spindle speed, cutting feed, feed rate, coolant flow and the axial depth of the cut are important.

Milling features

Benefits

  • With the right machine and tools, complex shapes can be obtained with great tolerances and high efficiency

Drawbacks

  • High investment costs with tools included
  • Higher production costs in application with more simple processing

Recommendations

The material of the workpiece, shape of the application and tolerances decides what kind of machine and tool that is needed.


SSAB Processing services Milling
Icon offer

Our offer 

SSAB Shape can offer machining services from our own centers globally and in addition we have a service partner network that can be utilized. Our offer includes:

  • Length up to 6000 mm
  • Width up to 2000 mm
  • Height up to 800 mm

In these service centers we have the possibility to combine milling of parts with other metal processing methods, for example press bending, to fulfil your complete requirements.

 