Product press releases

SSAB introduces Strenx 700 OME performance steel which meets ABS, DNV-GL and Lloyds Register classification rules

Strenx, Strenx 700 OME
May 02, 2016 8:00 CEST
Strenx 700 OME from SSAB provides the offshore industry with new opportunities to save weight and reduce welding costs.

The dual-certified Strenx 700 OME meets the standard requirements of ABS AB EQ70 / DNV-GL NVE 690 / LR EH69. In addition to the class approvals, SSAB has taken the workshop properties to a new level for this category of steels by also certifying the steel according to Strenx guarantees.

Strenx 700 OME / ABS AB EQ70
Strenx 700 OME / DNV-GL NVE 690
Strenx 700 OME / LR EH 69

Strenx guarantees represents SSAB’s ambition of enhancing our promise of workshop properties by offering exceptionally strict tolerances with regard to thickness tolerance, flatness tolerance and formability. The consistency in mechanical properties throughout the plate and from batch to batch is also something that characterizes Strenx performance steels. The improved tolerances and consistency also enable Strenx 700 OME to be used in cold formed profiles providing excellent production efficiency.

Strenx 700 OME guarantees the mechanical properties in the Z direction and can be ordered in compliance with the requirements of Z15, Z25, or Z35. Strenx 700 OME is an exceptionally clean steel that is guaranteed to meet the EN 10160 E1S1standard regarding impurities and porosity with the option to meet higher requirements in extra critical applications. The cleanness in combination with lean composition makes Strenx 700 OME easy to weld with retained properties.

By using Strenx 700 OME in offshore and marine structures there is a potential to save 30% on weight in comparison with a standard EH36 or S355 plate. Reducing the thickness can also save 50% in welding costs and in many cases will also reduce handling and installation costs.

The following applications are just some examples of how companies benefit from using Strenx 700 OME:

Gear racks and chords and pylons for jack-up legs and lift boats
Marine and offshore cranes and lifting devices
Pipe and cable-laying equipment
Ice breaking zones in hulls of service ships and ice breakers
Protection plates for subsea equipment
Green energy power plants as wave and tidal generators

For further information, please contact:
Joakim Nyström
Key Segment Manager – Energy & Offshore
SSAB Special Steels
M +46730892119
[email protected]

Ben Kowing
Marketing and Technical Support Director
SSAB Special Steels Americas
M +1 563 554 7103
[email protected]

For pictures, please visit SSAB’s Media bank

Attachments

SSAB introduces Strenx 700 OME performance steel which meets ABS, DNV-GL and Lloyds Register classification rules

Related articles

Product press releasesSSAB Expands Strenx® Certified Fabricator Network to the Netherlands
Strenx
Other press releasesSSAB and Putzmeister start partnership in fossil-free steel for concrete pumps and concrete mixers
Hardox, Strenx, SSAB Zero
Product press releasesHow Strenx® Weathering delivers cost-effective and maintenance-free corrosion protection
Strenx