Docol® 600LA high strength low alloy

Download data sheet

General Product Description

The Docol 600LA is a high-strength low-alloy steel that offer consistent properties for modern, rapid production methods. Typical applications include components and parts such as load-bearing structures, for example chassis. Docol HR600LA-UC can after agreement be adapted and delivered as dual certified with S600MC according to EN 10149-2.

Dimension Range

Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

Grade and coating specific restrictions on available dimensions may occur.

Mechanical Properties

Docol HR​600LA

Standard
SSAB
Coating
UC
Test direction
L
Yield strength Rp0.2
(MPa)
600 - 730
Tensile strength Rm
(MPa)
650 - 820
Elongation A80
(min %)
13 1)
Elongation A5
(min %)
16 2)
Min. inner bending radius for a 90° bend
1.1 x t

1) A80 value applies for thicknesses < 3.00 mm.

2) A5 value applies for thicknesses ≥ 3.00 mm.

Chemical Composition (ladle analysis)

Docol HR​600LA

Coating
UC
C
(max %)
0.12
Si
(max %)
0.60
Mn
(max %)
1.90
P
(max %)
0.025
S
(max %)
0.010
Al
(%)
From 0.015
Ti
(max %)
0.15
Nb
(max %)
0.09
Cu
(max %)
0.20

Tolerances

Hot rolled (UC): Tolerances in accordance to EN 10051.

Customized dimensional and shape tolerances are available upon request.

Surface Treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® High Strength Low Alloy steel product offer

Docol® 420LA high strength low alloy

Visualizza prodotto

Docol HR100XF

Visualizza prodotto

Docol HR110XF

Visualizza prodotto

Docol® S600MC high strength low alloy

Visualizza prodotto

Docol® S650MC high strength low alloy

Visualizza prodotto

Docol® S700MC high strength low alloy

Visualizza prodotto

Docol® S900MC high strength low alloy

Visualizza prodotto

Docol® 460LA high strength low alloy

Visualizza prodotto

Docol® 500LA high strength low alloy

Visualizza prodotto

Docol® 550LA high strength low alloy

Visualizza prodotto

Docol® 600LA high strength low alloy

Visualizza prodotto

Docol® 650LA high strength low alloy

Visualizza prodotto

Docol® 700LA high strength low alloy

Visualizza prodotto

Contenuti correlati

Stock di materiale di prova

Vuoi scoprire applicazioni automotive uniche nel loro genere, sperimentare nuovi metodi di produzione o creare componenti più leggeri che possano migliorare l'efficienza del carburante, la resistenza all'impatto dei veicoli e la sostenibilità?

Per saperne di più

Dati di formatura per gli acciai AHSS Docol®

Gli attuali clienti Docol® hanno accesso 24 ore su 24, 7 giorni su 7 ai dati di formatura necessari per aiutarli nella scelta e nella simulazione degli acciai altoresistenziali di nuova generazione per il settore automobilistico.

Per saperne di più