Tipper design > Sustainability of Hardox® in tipper bodies

Tipper body environmental considerations

A lighter vehicle made using less steel helps to reduce environmental impact by saving on primary energy resources and reducing greenhouse gas emissions.

In the life cycle assessment of a vehicle, different phases are often analyzed. When an upgraded dumper or trailer is compared to an original design in conventional steel, steel production and service life are dominating factors. The latter often accounts for 90% of the vehicle’s total environmental savings. When analyzing service life in the case of weight-limited cargo, the weight of the vehicle is considered. The fuel consumption of road vehicles depends on several resistance factors the vehicle has to overcome during its operation.

Except for aerodynamic resistance, all resistance factors are linearly dependent on vehicle mass. The aerodynamic resistance, however, depends on the vehicle’s dimensions and speed. Therefore, besides its mass, speed, acceleration and the gradient (hilly or flat) also affect the vehicle’s fuel consumption. These factors are highly dependent on the driving conditions and driving behavior. With the same driving conditions assumed, the correlation between fuel consumption and vehicle weight is linear, and the fuel savings corresponding to a specific weight savings is independent of the vehicle’s absolute weight.

Fast vehicles driven at a steady speed will have high aerodynamic resistance and low acceleration resistance, and thus moderate specific energy savings through weight reduction. Consequently, slow vehicles that have frequent stopping and acceleration will gain high fuel savings through weight reduction.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 