To evaluate the performance of different Hardox® grades, SSAB conducted wear tests with the addition of acetic acids to simulate household waste and other acid abrasive materials. The testing equipment consists of a drum machine with a diameter of 800 mm (31.5”). The drum houses 34 individual samples.

The drum wear test machine for 34 individual samples.

Inside the drum.

The drum was loaded with abrasive materials and liquid, and the samples were weighed both before and after the test to measure the weight loss of each sample. The run time was around 90 hours and the abrasive material was changed twice a day.
The weight loss of all the samples was then recalculated in order to calculate service life relative to Hardox® 450.

Relative service life based on material loss in the test drum.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026