This mining truck has been equipped with a body made of Hardox® 450. The weight of the new dump body is reduced by 2.5 tons or 25%, which can increase the maximum payload, while maintaining the same maximum vehicle weight. Additionally, the new body can have a longer lifetime than the conventional one.
Together with our customers, SSAB continually upgrades steel and equipment designs. SSAB EcoUpgraded saves CO2 both in steel production and during the full lifetime of the machine.
From the CO2 payback time and onwards, every extra hour brings additional savings.


| Calculation data | |
| Fuel consumption, fully loaded | 160 litres/hour |
| Fuel consumption, without load | 30 litres/hour |
| Machine usage per year | 3 000 hours/year |
| Distance with maximum load | 50 % |
| Service lifetime | 13 years |
| Maximum payload (before upgrading) | 96 000 kg |
| Gross weight (fully loaded) | 165 000 kg |
| Weight of original parts | 15 000 kg |
| Weight of upgraded parts | 12 500 kg |