GreenCoat RWS Pro BT

Download data sheet

General Product Description

GreenCoat RWS Pro BT color coated steel is available in matt finish. It provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat® products.

GreenCoat RWS Pro BT offers a high level of durability for rainwater systems using a double-sided coating (same coating is applied on both sides of the sheet).

GreenCoat RWS Pro BT color coated steel is optimized for weather and wear resistance. It provides good protection against corrosion (RC5) and mechanical abrasion as well as very good gloss retention and color fastness. GreenCoat RWS Pro BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

Excellent weather resistance together with regular maintenance and the cleaning of rainwater systems can maximize the service life of the product.

GreenCoat RWS Pro BT complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Technical Properties
Technical Properties
Gloss
Matt
10
Technical Properties
Technical Properties
Minimum inner bending radius
Matt
0.5 x sheet thickness
Technical Properties
Technical Properties
Scratch resistance
Matt
30 N
Technical Properties
Technical Properties
Lowest forming temperature
Matt
-15 °C
Technical Properties
Technical Properties
UV radiation resistance
Matt
RUV3
Technical Properties
Technical Properties
Corrosion resistance 1)
Matt
RC5
Technical Properties
Technical Properties
Stain resistance
Matt
Very good
Technical Properties
Technical Properties
Highest operating temperature
Matt
100 °C
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
Matt
35 µm
Technical Properties
Technical Properties
Coating structure
Matt
Structured
Technical Properties
Technical Properties
Steel designation 2)
Matt
FAX, PLX 3)
Technical Properties
Technical Properties
Zinc coating
Matt
275 g/m2
Technical Properties
Technical Properties
Min steel thickness 2)
Matt
0.50 mm
Technical Properties
Technical Properties
Steel width 2)
Matt
1000 - 1500 mm

1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

3) FAX fulfills the requirements of EN 10346 DX51D, PLX fulfills the requirements of EN 10346 DX54D.

Colors

Below are the colors currently available. Other colors can be agreed upon separately.

Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

The product may have slight tonal difference between batches and especially if their time of production differs significantly.

Reverse Side Coating

Same coating is applied on both sides of the sheet.

The technical properties apply for both sides. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

Reverse side stamping is not applicable for double sided products.