GreenCoat RWS Pro

Download data sheet

General Product Description

GreenCoat RWS Pro color coated steel is available in regular finish and offers a wide range of colors inspired by Nordic nature.

GreenCoat RWS Pro offers a high level of durability for rainwater systems using a double-sided coating (same coating is applied on both sides of the sheet).

GreenCoat RWS Pro color coated steel is optimized for weather and wear resistance. It provides good protection against corrosion (RC5) and mechanical abrasion as well as very good gloss retention and color fastness. GreenCoat RWS Pro possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

Excellent weather resistance together with regular maintenance and the cleaning of rainwater systems can maximize the service life of the product.

GreenCoat RWS Pro complies with current REACH regulations and is fully chromate-free.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Technical Properties
Technical Properties
Gloss
Regular
40
Technical Properties
Technical Properties
Minimum inner bending radius
Regular
0.5 x sheet thickness
Technical Properties
Technical Properties
Scratch resistance
Regular
30 N
Technical Properties
Technical Properties
Lowest forming temperature
Regular
-15 °C
Technical Properties
Technical Properties
UV radiation resistance
Regular
RUV3
Technical Properties
Technical Properties
Corrosion resistance 1)
Regular
RC5
Technical Properties
Technical Properties
Stain resistance
Regular
Very good
Technical Properties
Technical Properties
Highest operating temperature
Regular
100 °C
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
Regular
35 µm
Technical Properties
Technical Properties
Coating structure
Regular
Structured
Technical Properties
Technical Properties
Steel designation 2)
Regular
FAX, PLX 3)
Technical Properties
Technical Properties
Zinc coating
Regular
275 g/m2
Technical Properties
Technical Properties
Min steel thickness 2)
Regular
0.50 mm
Technical Properties
Technical Properties
Steel width 2)
Regular
1000 - 1500 mm

1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

2) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

3) FAX fulfills the requirements of EN 10346 DX51D, PLX fulfills the requirements of EN 10346 DX54D.

Colors

Below are the colors currently available. Other colors can be agreed upon separately.

Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

The product especially in metallic colors may have slight tonal difference between batches and especially if the time of production differs significantly.

Reverse Side Coating

Same coating is applied on both sides of the sheet.

The technical properties apply for both sides. However, different sides of the sheet cannot be mixed due to the possibility of a visual difference. The reverse side may show wider variation in color and gloss.

Reverse side stamping is not applicable for double sided products.

Contact Information

www.ssab.com/contact 