GreenCoat PLX Pro BT
Download data sheet
Download data sheet
GreenCoat PLX Pro BT color coated steel is available in regular and matt finishes and offers a wide range of colors inspired by Nordic nature. It uses a patented bio-based coating having Swedish rapeseed oil instead of traditional fossil oil in the paint, which is unique on the market. SSAB holds a worldwide patent for this coating technology (Bio-based Technology, BT).
This product has been developed together with tinsmiths in order to obtain optimum product properties combined with Nordic quality steel and an excellent coating. The result is a unique, premium product for tinsmiths.
GreenCoat PLX Pro BT color coated steel offers a high level of durability for standing-seam systems. It is highly formable, even by hand, and has practically no spring-back, which allows for very tight folding.
GreenCoat PLX Pro BT color coated steel offers a coating that is optimized to resist weathering, resulting in excellent corrosion resistance (RC5+). The product possesses excellent gloss retention and color fastness.
GreenCoat PLX Pro BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.
The reverse side of the sheet is painted with a two-layer Limestone Turquoise color backside coating.
GreenCoat PLX Pro BT complies with current REACH regulations and is fully chromate-free.
SSAB’s color coated steels are all manufactured according to EN 10169.
GreenCoat and PLX are trademarks of the SSAB group of companies.
1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after four years exposure in natural outdoor testing sites as specified in EN 10169.
2) PLX fulfills the requirements of EN 10346 DX54D.
3) Maximum steel thickness is 1.5 mm and maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.
Below are the colors currently available. Other colors can be agreed upon separately.
Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.
For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.
Colors
GreenCoat PLX Pro BT
Nordic White
RR1H3 / SS0020
Regular, Matt
Winter White
RR20 / SS0005
Regular
Snow White
RR19 / SS0001
Regular, Matt
Arctic White
RR1L6 / SS0002
Regular
Polar White
RR--- / SS6080
Matt
Powder White
RR--- / SS0021
Regular
Limestone Grey
RR268 / SS0022
Regular, Matt
Goosewing Grey
RR2H5 / SS0461
Regular
Gravel Grey
RR--- / SS0241
Matt
Quarry Grey
RR287 / SS0244
Regular, Matt
Rock Grey
RR237 / SS0061
Regular
Anthracite Grey
RR2H8 / SS0087
Regular, Matt
Mountain Grey
RR23 / SS0036
Regular, Matt
Summit Grey
RR--- / SS0454
Regular
Cliff Grey
RR288 / SS0455
Matt
Nordic Night Black
RR33 / SS0015
Regular, Matt
Walnut Brown
RR32 / SS0387
Regular, Matt
Acorn Brown
RR827 / SS0434
Regular, Matt
Coffee Brown
RR820 / SS0384
Regular, Matt
Cottage Red
RR29 / SS0758
Regular, Matt
Brick Red
RR7F2 / SS0742
Regular, Matt
Fire Brick Red
RR7G9 / SS0757
Matt
Harvest Yellow
RR24 / SS0189
Regular
Silver Fir Green
RR5J3 / SS0975
Regular, Matt
Leaf Green
RR594 / SS0874
Regular, Matt
Pine Green
RR11 / SS0830
Regular
Olive Leaf Green
RR5H8 / SS6033
Matt
Lake Blue
RR35 / SS0558
Regular
Metallic Silver
RR40 / SS0045
Regular, Matt
Metallic Sterling
RR974 / SS6045
Matt
Dark Silver Metallic
RR977 / SS6015
Matt
Metallic Dark Silver
RR41 / SS0044
Regular, Matt
Metallic Copper
RR979 / SS0778
Regular
Note for Metallic colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.
Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.
For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production year is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.