Hardenable boron steel for the automotive industry. Docol PHS 2000 steels are optimized for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as bumper systems, door impact beams, and B-pillar reinforcements.
Cold rolled / UC: thickness 1.00-2.10 mm, width up to 1515 mm.
Hot rolled / UC*: thickness 2.00-4.00 mm, width up to 1600 mm.
Slit strip and cut to length sheets are available upon request.
*Available upon request.
Standard | Condition | Test direction |
Typical yield strength Rp0.2 (MPa) |
Typical tensile strength Rm (MPa) | Typical elongation A80 (%) |
Typical elongation A5 (%) |
|
---|---|---|---|---|---|---|---|
Docol PHS FH 2000 | SSAB | Full Hard | T | 980 | 1100 | 4 | — |
Docol PHS CR 2000 Annealed | SSAB | As delivered Annealed | T | 330 | 530 | 26 | — |
SSAB | Hot stamped 1) | T | 1380 | 2040 | 5 | — | |
Docol PHS HR 2000 | SSAB | Hot rolled | T | 490 2) | 690 | 18 | 22 |
SSAB | Hot stamped 1) | T | 1360 2) | 2040 | 6 | 7 | |
Docol PHS HR 2000+A | SSAB | Annealed | T | 330 2) | 540 | 27 | 31 |
1) Properties depend on the process.
2) ReH is used instead of Rp0.2.
C (%) |
Si (%) |
Mn (%) |
P (max %) |
S (max %) |
Cr (max %) |
B (%) |
Nb+Ti (max %) |
---|---|---|---|---|---|---|---|
0.30 - 0.38 | 0.15 - 0.35 | 1.10 - 1.50 | 0.025 | 0.005 | 0.35 | 0.0010 - 0.0050 | 0.2 |
Cold rolled (UC): Tolerances in accordance to EN 10131.
Hot rolled (UC): Tolerances in accordance to EN 10051.
Customized dimensional and shape tolerances are available upon request.
Uncoated (UC): available as oiled.
All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.
Want to discover unique automotive applications for AHSS materials? Try new production methods? Or create lighter components that can improve fuel efficiency, crash-worthiness and sustainability?
Docol® steel grades serve specific design purposes and are chosen by designers for a wide range of applications and used by OEMs and tier suppliers in millions of vehicles around the world.
Existing Docol® customers get 24/7 access to the forming data you need to help in your selection and simulation of automotive advanced high strength steels.