Docol® PHS 1800 press hardening

Download data sheet

General Product Description

Docol PHS 1800 is cold rolled and alloyed with a small percentage of boron to improve hardenability. This steel is specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.

Slit strip and cut to length sheets are available upon request.

Mechanical Properties

Docol PHS FH 1800

Standard
SSAB
Condition
Full Hard
Test direction
T
Typical yield strength Rp0.2 (MPa)
970
Typical tensile strength Rm (MPa)
1070
Typical elongation A80
(%)
4

Docol PHS CR 1800 Annealed

Standard
SSAB
Condition
As delivered Annealed
Test direction
T
Typical yield strength Rp0.2 (MPa)
350
Typical tensile strength Rm (MPa)
500
Typical elongation A80
(%)
27

1) Properties depend on the process.

Chemical Composition (ladle analysis)

C
(%)
C
(%)
0.27 - 0.33
Si
(%)
0.15 - 0.35
Mn
(%)
1.00 - 1.45
P
(max %)
0.025
S
(max %)
0.010
Cr
(max %)
0.35
B
(%)
0.0008 - 0.0050

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Customized dimensional and shape tolerances are available upon request.

Surface treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® PHS steel product offer

Docol® PHS 1500 press hardening

View product

Docol® PHS 1800 press hardening

View product

Docol® PHS 2000 press hardening

View product

Related content

AHSS trial material stock

Want to discover unique automotive applications for AHSS materials? Try new production methods? Or create lighter components that can improve fuel efficiency, crash-worthiness and sustainability?

Read more

Automotive steel applications

Docol® steel grades serve specific design purposes and are chosen by designers for a wide range of applications and used by OEMs and tier suppliers in millions of vehicles around the world.

Read more

Forming data for Docol® AHSS steels

Existing Docol® customers get 24/7 access to the forming data you need to help in your selection and simulation of automotive advanced high strength steels.

Read more
Copyright 2026