General Product Description

A martensitic steel for automotive applications, Docol 1700M allows for increased crashworthiness, lightweight design and cost-efficient production methods for the automotive industry. Docol 1700M is one of the strongest cold rolled advanced high-strength steels on the market and has become the material of choice for automotive applications such as bumper systems and structural components.

Dimension Range

Cold rolled / UC: thickness 1.00-2.10 mm, width up to 1250 mm.

Mechanical Properties

Docol CR​1350Y​1700T-​MS

Standard
VDA 239-100
Coating
UC
Test direction
L
Yield strength Rp0.2
(MPa)
1350 - 1700
Tensile strength Rm
(MPa)
1700 - 2000
Elongation A80
(min %)
3
BH2
(min MPa)
30
Min. inner bending radius for a 90° bend
4.0 x t

Chemical Composition (ladle analysis)

Docol CR​1350Y​1700T-​MS

Coating
UC
C
(max %)
0.35
Si
(max %)
1.00
Mn
(max %)
3.00
P
(max %)
0.020
S
(max %)
0.010
Al
(%)
From 0.010
Nb+Ti
(max %)
0.15
Cr+Mo
(max %)
1.00
B
(max %)
0.010
Cu
(max %)
0.20

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Customized dimensional and shape tolerances are available upon request.

The following improved flatness tolerances are available for cold rolled martensitic products upon request. The tolerances are valid for mother coils only before slitting.

Thickness
(mmin)
Thickness
(mmin)
1.00 - 1.390.0394 - 0.0547
Max height 1)
(mm)
8
Thickness
(mmin)
Thickness
(mmin)
1.40 - 1.590.0551 - 0.0626
Max height 1)
(mm)
7
Thickness
(mmin)
Thickness
(mmin)
1.60 - 1.790.0630 - 0.0705
Max height 1)
(mm)
6
Thickness
(mmin)
Thickness
(mmin)
1.80 - 2.100.0709 - 0.0827
Max height 1)
(mm)
5

1) Distance from the top surface of the strip normal to flat surface. Measured with a ruler on sheets of mother coil width and minimum length 1200 mm. Cross bow and coil set excluded.

Surface Treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® Martensitic steel product offer

Docol® 900M martensitic

Visualizza prodotto

Docol® 1100M martensitic

Visualizza prodotto

Docol® 1200M martensitic

Visualizza prodotto

Docol® 1300M martensitic

Visualizza prodotto

Docol® 1400M martensitic

Visualizza prodotto

Docol® 1500M martensitic

Visualizza prodotto

Docol® 1700M martensitic

Visualizza prodotto

Contenuti correlati

Stock di materiale di prova

Vuoi scoprire applicazioni automotive uniche nel loro genere, sperimentare nuovi metodi di produzione o creare componenti più leggeri che possano migliorare l'efficienza del carburante, la resistenza all'impatto dei veicoli e la sostenibilità?

Per saperne di più

Dati di formatura per gli acciai AHSS Docol®

Gli attuali clienti Docol® hanno accesso 24 ore su 24, 7 giorni su 7 ai dati di formatura necessari per aiutarli nella scelta e nella simulazione degli acciai altoresistenziali di nuova generazione per il settore automobilistico.

Per saperne di più