SSAB Polyester / Zero

Download data sheet

General Product Description

SSAB Polyester color coated steel with SSAB Zero™ - also called SSAB Polyester / Zero - is available with SSAB S280GD Zero. SSAB Zero™ steel is made using recycled steel and fossil-free energy. 

The SSAB Zero™ EPDs and Certificate of Carbon Emissions is available on ssab.com. The availability of SSAB Zero™ products is subject to limitations and conditions of delivery have to be agreed upon separately. Note: Emissions from the painting process of color coated products are not included in the SSAB Zero™ Certificate of Carbon Emissions.

SSAB S280GD Zero is manufactured according to EN 10346.

 

SSAB Polyester with SSAB Zero™ is available for indoor applications like sandwich panel indoor walls. SSAB Polyester possesses good weather resistance properties (RC3) and offers a smooth surface and a good flexibility when processing. The typical gloss level is regular gloss, but other glosses are available from request.

The reverse side of the sheet is painted with a two-layer grey backside coating.

SSAB Polyester complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

Technical Properties

Technical Properties
Technical Properties
Gloss
Regular
35
Technical Properties
Technical Properties
Minimum inner bending radius
Regular
3 x sheet thickness
Technical Properties
Technical Properties
Scratch resistance
Regular
20 N
Technical Properties
Technical Properties
UV radiation resistance
Regular
RUV2-3
Technical Properties
Technical Properties
Corrosion resistance 1)
Regular
RC3
Technical Properties
Technical Properties
Stain resistance
Regular
Satisfactory
Technical Properties
Technical Properties
Highest operating temperature
Regular
90 °C
Technical Properties
Technical Properties
Fire classification, EN 13501-1
Regular
A1 s1 d0
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
Regular
25 µm
Technical Properties
Technical Properties
Coating structure
Regular
Smooth
Technical Properties
Technical Properties
Steel designation 2)
Regular
S280GD Zero, S350GD Zero*, DX51D Zero*, HX340LAD Zero*
Technical Properties
Technical Properties
Zinc coating
Regular
275 g/m2
Technical Properties
Technical Properties
Min steel thickness 2)
Regular
0.42 mm
Technical Properties
Technical Properties
Steel width 2)
Regular
1000 - 1500 mm
* Trial deliveries

1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

2) Maximum steel thickness for SSAB S280GD Zero is 0.75 mm. Maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

Colors

Below are the colors currently available. Other colors can be agreed upon separately.

Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

Reverse Side Coating

Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

Technical Properties
Technical Properties
Nominal Coating Thickness (primer + top coat)
12 µm
Technical Properties
Technical Properties
Color
Grey
Technical Properties
Technical Properties
Corrosion Resistance
Min CPI3

For easy material identification the reverse side of the sheet is stamped with the SSAB logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.

Protective Film

Temporary protective films are available for protection during processing and installation. Protective films are applied on the top side of the Product. Films will be centered to the strip meaning that typically there are small unprotected areas in both edges of the strip. Unprotected area may be cut away if customer so wishes. Joined film strip ends are marked with red tape on the edge of the product.

Products with protective film should be stored in dry and warm conditions, since the adhesion between protective film and color coating decreases both in high and low temperatures. Humidity changes also the adhesion properties and in worst case leaves the adhesive part of the film on the product surface.

Adhesion of protective film increases over time, eventually making it difficult to remove the film from the Product’s surface. Due to that, protective film is recommended to be removed from the material as soon as possible, but no later than six months from the manufacturing of the Product or after one month from the end product installation depending on which comes first.

Protective film decreases friction between coil windings, which creates a high risk of coil collapsing on thin gauge coils. Due to the risk of collapsing, SSAB does not recommend protective films for steel nominal thickness ≤ 0,60 mm. If protective film is essential, following precautions must be taken to minimize the risk of collapsing: Max coil weight < 5 tons and self-supporting coil protection shields must be used in the package.

Typical protective film thickness is around 45µm, max working temperature +80°C and max and min stripping temperatures +40°C & -10°C.

Protective film has a good resistance to forming but is susceptible to cuts. When working with material with a protective film, clean tools that do not damage the film, and appropriate methods are to be used. Cutting fluids are not needed because the film protects the material surface and reduces friction. Cutting fluids may also have negative impact on the protective film and its adhesion.

Protective films can be recycled as plastics, combusted or disposed via the municipal waste management system depending on the local waste management guidelines and regulations.