Det Norske Veritas

The Det Norske Veritas, DNV, specifications identify the general requirements for normal, high or extra high strength hot rolled plates up to 150 mm in thickness to be used in the construction of hulls and other marine structures.

Show specs in Imperial Metric
Hide/Show specific columns Edit
Select columns to display
    Product Name Dimensions Datasheet
    NV A/B/D/E T: 0.1875 - 5.91 inches
    L: 154 - 1020 inches
    W: 72 - 129.9 inches
    T: 4.762 - 150 mm
    L: 3910 - 25910 mm
    W: 1800 - 3299 mm
    NV A/D/E 32 T: 0.1969 - 5.91 inches
    L: 79 - 906 inches
    W: 75 - 129.9 inches
    T: 5.001 - 150 mm
    L: 2000 - 23000 mm
    W: 1900 - 3299 mm
    NV A/D/E 36 T: 0.1875 - 2.00 inches
    L: 240 - 1020 inches
    W: 72 - 120 inches
    T: 4.762 - 50.8 mm
    L: 6100 - 25910 mm
    W: 1800 - 3050 mm
    NV A/D/E 40 T: 0.2362 - 1.575 inches
    L: 79 - 906 inches
    W: 75 - 129.9 inches
    T: 5.999 - 40.00 mm
    L: 2000 - 23000 mm
    W: 1900 - 3299 mm
    NV D/E 460 T: 0.7874 - 2.362 inches
    L: 79 - 906 inches
    W: 75 - 129.9 inches
    T: 20.00 - 59.99 mm
    L: 2000 - 23000 mm
    W: 1900 - 3299 mm
    NV A/D/E 500 T: 0.3937 - 1.574 inches
    L: 79 - 906 inches
    W: 75 - 129.9 inches
    T: 10.00 - 39.98 mm
    L: 2000 - 23000 mm
    W: 1900 - 3299 mm
    Compare parameters

    Select one parameter to compare

    Comparison