SSAB Laser® 420MC Plus

Download data sheet

Select Language

    General Product Description

    SSAB Laser® 420MC Plus is an advanced high yield strength cold forming steel for laser cutting. The SSAB guarantee for flatness, both before and after laser cutting, is ≤ 3 mm/m deviation.

    SSAB Laser® 420MC Plus meets and exceeds the requirements of S420MC in EN 10149-2. Upon agreement, it can be delivered as dual certified. This dual certification will enable producers of steel structures, in accordance with EN 1090, to use SSAB Laser® 420MC Plus in their CE-marked final component or structure.

    Dimension Range

    Hide/Show specific columns Edit
    Select columns to display
      Delivery form Thickness
      (mm)
      Width
      (mm)
      Length
      (mm)
      Hot rolled sheet as rolled 3.0 - 12.0 1000 - 1860 1000 - 16000
      Hot rolled sheet pickled and oiled 3.0 - 10.0 1000 - 1860 1000 - 16000
      Compare parameters

      Select one parameter to compare

      Comparison

        Mechanical Properties

        Hide/Show specific columns Edit
        Select columns to display
          Yield strength ReH
          (min MPa)
          Tensile strength Rm
          (MPa)
          Elongation A80 1)
          (min %)
          Elongation A5 2)
          (min %)
          Min. inner bending radius for a 90° bend 3)
          (x t)
          420 490 - 620 16 21 0.0
          Compare parameters

          Select one parameter to compare

          Comparison

            The mechanical properties are tested in the longitudinal direction.

            1) A80 value applies for thicknesses < 3.00 mm.

            2) A5 value applies for thicknesses ≥ 3.00 mm.

            3) The bending guarantee is valid for both longitudinal and transverse direction.

            Impact Properties

            Hide/Show specific columns Edit
            Select columns to display
              Min. impact energy for longitudinal testing,
              Charpy V 10x10 mm test specimens
              40 J / -60 °C
              Compare parameters

              Select one parameter to compare

              Comparison

                Min. impact energy for longitudinal testing,
                Charpy V 10x10 mm test specimens
                40 J / -60 °C
                Impact testing according to EN ISO 148-1 is performed on thicknesses ≥ 6mm. The specified minimum value corresponds to a full-size specimen.

                Chemical Composition (ladle analysis)

                Hide/Show specific columns Edit
                Select columns to display
                  C
                  (max %)
                  Si
                  (max %)
                  Mn
                  (max %)
                  P
                  (max %)
                  S
                  (max %)
                  CEV
                  (max )
                  0.12 0.03 1.5 0.020 0.015 0.28
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    All SSAB Laser® steels are aluminum-killed (Al ≥ 0.015%) and grain-refined. Additionally, niobium (Nb), vanadium (V), titanium (Ti) and/or boron (B) may be used as single alloying element or in any combination.

                    Tolerances

                    All SSAB Laser® products are delivered with SSAB Laser® tolerances, which means increased guarantees compared to corresponding EN standards. Detailed information is available on ssab.com.

                    Thickness

                    Hot rolled sheet: SSAB Laser® tolerances correspond to ⅔ of EN 10051 as default. Tighter tolerances are available upon request.

                    Width

                    Hot rolled sheet: -0/+20 mm for mill edge sheet; -0/+2 mm for cut edge sheet. Tighter tolerances are available upon request.

                    Length

                    Hide/Show specific columns Edit
                    Select columns to display
                      Nominal length
                      (mm)
                      Tolerance
                      (mm)
                      l ≤ 4000 - 0 / + 3
                      4000 ˂ l ≤ 6000 - 0 / + 4
                      6000 ˂ l ≤ 8000 - 0 / + 5
                      8000 ˂ l ≤ 13000 - 0 / + 6
                      13000 ˂ l ≤ 16000 - 0 / + 8
                      Compare parameters

                      Select one parameter to compare

                      Comparison

                        Nominal length
                        (mm)
                        l ≤ 4000
                        Tolerance
                        (mm)
                        - 0 / + 3
                        Nominal length
                        (mm)
                        4000 ˂ l ≤ 6000
                        Tolerance
                        (mm)
                        - 0 / + 4
                        Nominal length
                        (mm)
                        6000 ˂ l ≤ 8000
                        Tolerance
                        (mm)
                        - 0 / + 5
                        Nominal length
                        (mm)
                        8000 ˂ l ≤ 13000
                        Tolerance
                        (mm)
                        - 0 / + 6
                        Nominal length
                        (mm)
                        13000 ˂ l ≤ 16000
                        Tolerance
                        (mm)
                        - 0 / + 8

                        Shape

                        According to EN 10051.

                        Flatness

                        ≤ 3 mm/m flatness deviation for both delivery condition and laser cut parts.

                        Surface Properties

                        According to EN 10163-2 Class A, Subclass 3.

                        Delivery Conditions

                        Thermomechanically rolled.

                        Surface and edge condition

                        SSAB Laser® MC Plus products are available in as rolled or pickled and oiled surface condition with mill edge. Cut edge sheets are available upon request.

                        Fabrication and Other Recommendations

                        All SSAB Laser® products have been optimized for laser cutting, cold forming and welding.

                        SSAB Laser® MC Plus products are cold forming steels not suited for heat treatments at temperatures above 580°C, since the material then may lose its guaranteed properties.

                        For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.