Docol® PHS 2000 press hardening

Download data sheet

General Product Description

Hardenable boron steel for the automotive industry. Docol PHS 2000 steels are optimized for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as bumper systems, door impact beams, and B-pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 1.00-2.10 mm, width up to 1515 mm.

Hot rolled / UC*: thickness 2.00-4.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

*Available upon request.

Mechanical Properties

Docol PHS FH 2000

Standard
SSAB
Condition
Full Hard
Test direction
T
Typical yield strength Rp0.2 (MPa)
980
Typical tensile strength Rm (MPa)
1100
Typical elongation A80
(%)
4
Typical elongation A5
(%)
—

Docol PHS CR 2000

Docol PHS HR 2000+A

Standard
SSAB
Condition
Annealed
Test direction
T
Typical yield strength Rp0.2 (MPa)
330 2)
Typical tensile strength Rm (MPa)
540
Typical elongation A80
(%)
27
Typical elongation A5
(%)
31

1) Properties depend on the process.

2) ReH is used instead of Rp0.2.

Chemical Composition (ladle analysis)

C
(%)
C
(%)
0.30 - 0.38
Si
(%)
0.15 - 0.35
Mn
(%)
1.10 - 1.50
P
(max %)
0.025
S
(max %)
0.005
Cr
(max %)
0.35
B
(%)
0.0010 - 0.0050
Nb+Ti
(max %)
0.2

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Hot rolled (UC): Tolerances in accordance to EN 10051.

Customized dimensional and shape tolerances are available upon request.

Surface Treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® PHS steel product offer

Docol® PHS 1500 press hardening

Wyświetl produkt

Docol® PHS 1800 press hardening

Wyświetl produkt

Docol® PHS 2000 press hardening

Wyświetl produkt

Powiązane dokumenty

Magazyn materiałów próbnych

Chcesz poznać unikalne zastosowania, wypróbować nowe metody produkcji czy opracować lżejsze komponenty, które poprawią ekonomikę paliwową, wytrzymałość antyzderzeniową i zrównoważony rozwój?

Dowiedz się więcej

Dane dotyczące formowania stali AHSS Docol®

Klienci stosujący Docol® otrzymują całodobowy dostęp do danych dotyczących formowania, pomagających w wyborze materiałów i symulacji procesów produkcji komponentów z zaawansowanej stali motoryzacyjnej o wysokiej wytrzymałości.

Dowiedz się więcej