SSAB Docol PHS 1800 is cold rolled and alloyed with a small percentage of boron to improve hardenability. This steel is specially developed for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as door impact beams, bumper systems and B- pillar reinforcements.
Cold rolled / UC: thickness 0.70-3.00 mm, width up to 1500 mm.
Slit strip and cut to length sheets are available upon request.
Docol PHS FH 1800
Docol PHS CR 1800
1) Properties depend on the process.
Cold rolled (UC): Tolerances in accordance to EN 10131.
Customized dimensional and shape tolerances are available upon request.
Uncoated (UC): available as oiled.
All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.