Your guide to Hardox® wear steel products

From abrasion-resistant wear plate to cut-to-length sheet, tubes, pipes and round bars, Hardox® steel answers all your wear challenges. Here’s your guide to the wide range of Hardox® products.

Show specs in:

ImperialMetric

Locally available from a worldwide network

Local availability on a global scale, a fast-track supply chain and personal commitment help ensure that you get Hardox® wear steel when and where you need it. With quick access to Hardox® wear plate on your local market, you can free up warehouse space and minimize capital tied up in inventory. The most common Hardox® grades and dimensions can reach you within 48 hours, directly from an SSAB mill or from local SSAB stocks.

Find your local stock

Technical support and beyond, at your service 24/7

Your needs. Your applications. In your language. Our local teams of experts are passionate about helping you find the right Hardox® product, offering you design and development support, and making you more productive, whether on the job or in the workshop. Whatever you build, we’ll help make sure your equipment gives you optimal productivity, maximum service life and unbeatable performance.

Contact our support team

Hardox® 400, Hardox® 450 and Hardox® 500 Tuf wear steels with structural properties

Hardox® 500 Tuf is the world’s hardest wear plate with structural properties. It delivers high strength, high hardness and guaranteed toughness in a single wear plate – a truly outstanding material for the most demanding applications. It has proved itself worldwide in truck and tipper bodies, containers, mining dumpers, buckets and other attachments, agricultural equipment, liners and wear parts. Thanks to its toughness, it can perform as a structural material in recycling containers, dump bodies, buckets and other heavy-duty products, even in freezing conditions. Combining the best properties from Hardox® 450 and Hardox® 500, it’s your go-to wear plate with no real competition on the market.

Hardox® 450 has a solid reputation as a highly versatile, abrasion-resistant steel that also has structural properties. With an extra 50 HBW hardness over AR 400 grades, it provides additional wear resistance for an extended service life. The hardness also increases the steel’s strength, with better dent resistance as a result. The high toughness also in cold conditions ensures that equipment can take impact forces without compromising its structural integrity.

Hardox® 400 is an all-around wear resistant steel with a nominal hardness of 400 HBW. It’s well suited for moderate wear applications that require high toughness, good bendability and excellent weldability.

Product Name

Hardox® 400

Thickness range (inmm)
0.079 - 5.1182.0 - 130.0
Hardness (HBW)
370 - 430
Typical CET (CEV)
0.24 - 0.41 (0.39 - 0.89)
Transverse test, guaranteed impact energy /
Longitudinal test, typical impact energy
LT: 33 ft-lbs / -40 °FLT: 45 J / -40 °C
Datasheet
Product Name

Hardox® 450

Thickness range (inmm)
0.031 - 6.2990.8 - 160.0
Hardness (HBW)
425 - 475
Typical CET (CEV)
0.32 - 0.40 (0.45 - 0.71)
Transverse test, guaranteed impact energy /
Longitudinal test, typical impact energy
LT: 37 ft-lbs / -40 °FLT: 50 J / -40 °C
Datasheet
Product Name

Hardox® 500 Tuf

Thickness range (inmm)
0.079 - 1.5002.0 - 38.1
Hardness (HBW)
475 - 505
Typical CET (CEV)
0.35 - 0.40 (0.52 - 0.59)
Transverse test, guaranteed impact energy /
Longitudinal test, typical impact energy
TT: 20 ft-lbs / -40 - -4 °F LT: 33 ft-lbs / -40 °FTT: 27 J / -40 - -20 °C LT: 50 J / -40 °C
Datasheet

Hardox® 500 and Hardox® 550 for challenging wear conditions

These abrasion-resistant steels are targeted at severe wear applications requiring limited structural performance. Hardox® 500 has a nominal hardness of 500 HBW for long service life while maintaining good processability and toughness. Hardox® 500 is used in applications such as liner plates, grizzly bars, wear bars and other wear parts in wear-intense industries.

Hardox® 550 has a nominal hardness of 550 HBW and toughness close to Hardox® 500. It gives higher wear resistance, but not at the expense of crack integrity. Hardox® 550 offers wear life improvements when replacing lower hardness steel grades or manganese steels. Typical applications include liner plates for crushers, chutes and other processing equipment, or hammers in recycling.

Product Name

Hardox® 500

Thickness range (inmm)
0.079 - 4.0552.0 - 103.0
Hardness (HBW)
470 - 530
Typical CET (CEV)
0.37 - 0.48 (0.50 - 0.86)
Transverse test, guaranteed impact energy /
Longitudinal test, typical impact energy
LT: 27 ft-lbs / -40 °FLT: 37 J / -40 °C
Datasheet
Product Name

Hardox® 550

Thickness range (inmm)
0.315 - 2.5598.0 - 65.0
Hardness (HBW)
525 - 575
Typical CET (CEV)
0.46 - 0.58 (0.67 - 0.79)
Transverse test, guaranteed impact energy /
Longitudinal test, typical impact energy
LT: 22 ft-lbs / -40 °FLT: 30 J / -40 °C
Datasheet

Hardox® 600 for superior wear resistance

Hardox® 600 has a nominal hardness of 600 HBW and a uniquely high toughness for such a hard steel. While targeted at more severe wear conditions, Hardox® 600 can still be cut and welded, making it an excellent choice for high-performance applications. Hardox® 600 has been successfully used in cement plants for concrete brick molds, tables and compactors; as liner plates and screed plates in material handling and mineral processing; as liners for stationary concrete mixers; and as hammers and knives in recycling and waste fragmentation.

Product Name

Hardox® 600

Thickness range (inmm)
0.098 - 2.5592.5 - 65.0
Hardness (HBW)
550 - 640
Datasheet

Hardox® Extreme takes wear resistance to the extreme

Hardox® Extreme is the world’s hardest wear plate with a nominal hardness of 60 HRC (Rockwell) and a typical hardness of 650-700 HBW. Hardox® Extreme is intended for applications with extremely high demands on abrasion resistance, such as liner plates. In glass recycling equipment, Hardox® Extreme both reduces lifecycle cost and extends service life without degrading the finished product.

Product Name

Hardox® Extreme

Thickness range (inmm)
0.315 - 0.7488.0 - 19.0
Hardness (HRC)
57 - 63
Datasheet

Hardox® HiTuf for the thickest structural wear applications

Hardox® HiTuf is an abrasion-resistant steel plate with guaranteed impact toughness of 40 J at -40°C (-40°F). Hardox® HiTuf steel with a nominal hardnessof 350 HBW makes a perfect choice for thick plate applications demanding extreme toughness and structural properties. It can in many cases replace castings or cast parts. It is commonly used as a structural wear part for thick cutting edges for large mining buckets and shovels, demolition tools and rippers, and where wear bars and shrouds protect the underlying structure.

Product Name

Hardox® HiTuf

Thickness range (inmm)
1.575 - 6.29940.0 - 160.0
Hardness (HBW)
310 - 370
Typical CET (CEV)
0.36 - 0.39 (0.55 - 0.64)
Min impact energy, transverse test
-
Datasheet

Hardox® HiAce for wear, corrosion, and high temperatures

Hardox® HiAce is a wear-resistant steel designed for demanding applications where corrosive or elevated-temperature conditions accelerate wear. Typical uses include garbage trucks, containers and recycling facilities, pulp and paper processing, sawmills, waste-to-energy plants and biomass plants, as well as mining and other process industries. It is also suitable for high-temperature equipment in industries like asphalt production, steelmaking, power generation and foundries. With a nominal hardness of 450 HBW, Hardox® HiAce provides the same excellent performance as Hardox® 450 while delivering reliable wear resistance in these environments.

Product Name

Hardox® HiAce

Thickness range (inmm)
0.118 - 3.9373.0 - 100.0
Typical CET (CEV)
0.38 - 0.39 (0.99 - 1.01)
Transverse test, guaranteed impact energy /
Longitudinal test, typical impact energy
TT: 20 ft-lbs / -4 °FTT: 27 J / -20 °C
Datasheet

Hardox® round bars

Hardox® round bars offer a through-thickness hardness with excellent toughness values. Hardox® round bars combine a high nominal hardness (400 HBW), toughness and weldability in a way that makes them unique in the market. They come in a wide range of dimensions and feature the same properties as the wear plate. Typical applications include wear parts and components for harvesters, sieving buckets, agricultural machinery, pins, rods, axels, and other components for buckets and machinery in construction, material handling and mineral processing, mining and drilling. In short, it makes a great fit in applications requiring a round steel bar that offers high wear resistance and good weldability.

Product Name

Hardox® Round bar

Diameter (mm)
40.00 - 160.040.0 - 160.0
Hardness (HBW)
370 - 540
Typical CET (CEV)
0.37 - 0.48 (0.58 - 0.95)
Longitudinal test, typical impact energy
27 - 45 J / -40 - -20 °F27 - 45 J / -40 - -20 °C
Min. impact energy for longitudinal testing
20 - 27 J / -40 °C27 J / -40 °C
Datasheet

Hardox® tubes and pipes

Hardox® tubes and pipes provide extreme performance and extended service life. Hardox® 400 tubes and pipes have a nominal hardness of 400 HBW, while Hardox® 500 tubes and pipes have a nominal hardness of 500 HBW. Both are great choices when you need high wear resistance and a lighter product. Hardox® tubes are used for transporting all types of abrasive materials, such as wet concrete, soil, gravel, ore slurry and iron ore pellets in steel mills. They can replace costly wear products like hard-faced overlay pipes and high chrome white iron.

Product Name

Hardox® Tubes & Pipes

Dimensions (mm)
Circular: 76.2 - 219.2
Wall thickness: 3.00 - 5.99
Mill length: 5999.99
Circular: 76.1 - 219.1
Wall thickness: 3.0 - 6.0
Mill length: 6000
Hardness (HBW)
360 - 530
Datasheet