API Line Pipe Steels

SSAB produces five API Line Pipe grades of steel. These API grades are typically used for transporting liquid petroleum and natural gas.

Show specs in:

ImperialMetric
Product Name

API 5L Grade X42

Dimensions
T: 0.250 - 1.00 in
L: 500 in
W: 60 - 120 in
T: 6.35 - 25.4 mm
L: 12700 mm
W: 1500 - 3050 mm
Datasheet
Product Name

API 5L Grade X52

Dimensions
T: 0.250 - 1.00 in
L: 500 in
W: 60 - 120 in
T: 6.35 - 25.4 mm
L: 12700 mm
W: 1500 - 3050 mm
Datasheet
Product Name

API 5L Grade X60

Dimensions
T: 0.250 - 0.875 in
L: 500 in
W: 60 - 120 in
T: 6.35 - 22.2 mm
L: 12700 mm
W: 1500 - 3050 mm
Datasheet
Product Name

API 5L Grade X65

Dimensions
T: 0.250 - 0.771 in
L: 500 in
W: 60 - 120 in
T: 6.35 - 19.6 mm
L: 12700 mm
W: 1500 - 3050 mm
Datasheet
Product Name

API 5L Grade X70

Dimensions
T: 0.345 - 0.771 in
L: 500 in
W: 60 - 120 in
T: 8.76 - 19.6 mm
L: 12700 mm
W: 1500 - 3050 mm
Datasheet
Product Name

API 5L Grade B

Dimensions
T: 0.250 - 1.00 in
L: 500 in
W: 60 - 120 in
T: 6.35 - 25.4 mm
L: 12700 mm
W: 1500 - 3050 mm
Datasheet