API 5L Grade X70

Download data sheet

General Product Description

API Specification 5L is the American Petroleum Institute’s specification for seamless and welded line pipe for use in petroleum transportation systems in the petroleum and natural gas industries. SSAB produces plate and coil skelp (the input material to a pipe manufacturing operation) for conversion by a pipe mill into welded line pipe. The specific type of pipe manufacturing operation may alter the mechanical properties of the skelp and consequently orders for skelp by pipe mills are typically each unique relative to the specified skelp quality level, delivery condition, chemical composition limits, and the specified as-delievered skelp properties based on the pipe manufacturing operation and the intented application for the line pipe. As a result, all inquiries for skelp orders are subjected to review. In the pipe body, API 5L Grade X70 pipe has a specified minimum yield strength of 70.3 ksi.

Available Dimensions

All orders are subject to review for applicability for specific pipe manufacturing method. Inquire for other thickness, width, or plate length availability.

Grade
Grade
Grade X70
Product type
Coils
Thickness
(in)
0.345 - 0.665
Width
(in)
60 - 96
Length
(in)
—
Grade
Grade
Grade X70
Product type
Plate
Thickness
(in)
0.375 - 0.771
Width
(in)
60 - 120
Length
(in)
500

Mechanical Properties

Grade
Grade
Grade X70
0.2% YS
(ksi)
0 1)
UTS
(ksi)
0 1)
Elongation in 2"
(min %)
0 1)
Elongation in 8"
(min %)
0 1)
Grade
Grade
Grade X70
0.2% YS
(ksi)
0 1)
UTS
(ksi)
0 1)
Elongation in 2"
(min %)
0 1)
Elongation in 8"
(min %)
0 1)

1) Inquire for mechanical properties requirements for coil and plate skelp.

Chemical Composition

Composition meets PSL2 (X65M) requirements. Inquire for SSC/HIC performance.

Grade
Grade
Grade X70
C
(max wt %)
0.12
Mn 1)
(max wt %)
1.70
P
(max wt %)
0.025
S
(max wt %)
0.015
Si
(max wt %)
0.45
Cu
(max wt %)
0.50
Ni
(max wt %)
0.50
Mo
(max wt %)
0.50

1) For each reduction of 0.01% below the specified maximum for C, an increase of 0.05% above the specified maximum for Mn is permitted, up to a maximum of 2.00%.

Carbon Equivalent

Composition meets PSL2 (X70M) requirements.

Grade
Grade
Thickness (in)
Grade X70
0.345 - 0.771
Grade
Grade
CEIIW (max wt %)
Grade X70
0.43
Grade
Grade
Pcm (max wt %)
Grade X70
0.25