SSAB Laser® 355C is an advanced structural cold forming steel for laser cutting. The SSAB guarantee for flatness, both before and after laser cutting, is ≤ 3 mm/m deviation.
SSAB Laser® 355C meets and exceeds the requirements of S355K2C+N in EN 10025-2. Dual certification and CE marking are available upon request.
Delivery form | Thickness (mm) |
Width (mm) |
Length (mm) |
---|---|---|---|
Hot rolled sheet as rolled | 3.0 - 15.0 | 1000 - 1860 | 1000 - 16000 |
Hot rolled sheet pickled and oiled | 3.0 - 15.0 | 1000 - 1830 | 1000 - 16000 |
Hot rolled plate as rolled | 8.0 - 30.0 | 1000 - 3300 | 2000 - 15000 |
Delivery form | Thickness (mm) |
Yield strength Re (min MPa) |
Tensile strength Rm (MPa) |
Elongation A5 (min %) |
Min. inner bending radius 90° t ≤ 6mm 1) (x t) |
Min. inner bending radius 90° t ˃ 6mm 1) (x t) |
---|---|---|---|---|---|---|
Hot rolled sheet | 3.0 - 15.0 | 355 | 490 - 630 | 20 | 1.5 | 1.5 |
Hot rolled plate | 8.0 - 30.0 | 355 | 490 - 630 | 20 | — | 1.5 |
The mechanical properties are tested transverse to the direction of rolling.
1) The bending guarantee is valid for both longitudinal and transverse direction.
Min. impact energy for longitudinal testing, Charpy V 10x10 mm test specimens |
---|
40 J / -20 °C |
Delivery form | C (max %) |
Si (max %) |
Mn (max %) |
P (max %) |
S (max %) |
CEV (max ) |
---|---|---|---|---|---|---|
Hot rolled sheet | 0.18 | 0.03 | 1.6 | 0.020 | 0.020 | 0.45 |
Hot rolled plate | 0.2 | 0.03 | 1.6 | 0.020 | 0.020 | 0.45 |
All SSAB Laser® steels are aluminum-killed (Al ≥ 0.015%) and grain-refined. Additionally, niobium (Nb), vanadium (V), titanium (Ti) and/or boron (B) may be used as single alloying element or in any combination.
All SSAB Laser® products are delivered with SSAB Laser® tolerances, which means increased guarantees compared to corresponding EN standards. Detailed information is available on ssab.com.
Hot rolled sheet: SSAB Laser® tolerances correspond to ⅔ of EN 10051 as default. Tighter tolerances are available upon request.
Hot rolled plate: SSAB Laser® tolerances correspond to ¾ of EN 10029 as default.
Hot rolled sheet: -0/+20 mm for mill edge sheet; -0/+2 mm for cut edge sheet. Tighter tolerances are available upon request.
Hot rolled plate: -0/+4-10mm depending on the thickness.
Nominal length (mm) |
Tolerance (mm) |
---|---|
l ≤ 4000 | - 0 / + 3 |
4000 ˂ l ≤ 6000 | - 0 / + 4 |
6000 ˂ l ≤ 8000 | - 0 / + 5 |
8000 ˂ l ≤ 13000 | - 0 / + 6 |
13000 ˂ l ≤ 16000 | - 0 / + 8 |
Nominal length (mm) |
Tolerance (mm) |
---|---|
2000 ˂ l ≤ 10000 | - 0 / + 15 |
10000 ˂ l ≤ 15000 | - 0 / + 20 |
Hot rolled sheet: according to EN 10051.
Hot rolled plate: according to EN 10029.
Hot rolled sheet: ≤ 3 mm/m flatness deviation for both delivery condition and laser cut parts.
Hot rolled plate: ≤ 3 mm/m flatness deviation for both delivery condition and laser cut parts.
According to EN 10163-2 Class A, Subclass 3.
Normalized rolled.
Hot rolled sheet: as rolled or pickled and oiled surface condition with mill edge. Cut edge is available upon request.
Hot rolled plate: as rolled surface condition and cut edges as default.
All SSAB Laser® products have been optimized for laser cutting, cold forming and welding.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.