GreenCoat Pro BT / Zero

Download data sheet

General Product Description

GreenCoat Pro BT with SSAB Zero™ - also called GreenCoat Pro BT / Zero - is available with S280GD Zero. SSAB Zero™ steel is made using recycled steel and fossil-free energy. 

The SSAB Zero™ EPDs and Certificate of Carbon Emissions is available on ssab.com. The availability of SSAB Zero™ products is subject to limitations and conditions of delivery have to be agreed upon separately. Note: Emissions from the painting process of color coated products are not included in the SSAB Zero™ Certificate of Carbon Emissions.

S280GD Zero is manufactured according to EN 10346.

 

GreenCoat Pro BT / Zero is available in regular and matt finishes. It provides a coating where rapeseed oil and other renewable raw materials are used. SSAB has long experience of Bio-based Technology (BT) in GreenCoat® products.

GreenCoat Pro BT is highly durable and has mainly been developed for roofing applications like profiled roof tiles or standing seam systems.

GreenCoat Pro BT possesses excellent forming properties enabling very demanding folding even down to -15°C, allowing for year round installation at lower costs.

GreenCoat Pro BT color coated steel is also optimized for wear resistance, weathering resistance and low resource consumption. It has greater durability than standard polyester products when exposed to people walking on the roof and other roof stresses. The product possesses excellent gloss retention and color fastness. It also provides good protection against corrosion reaching the highest RC5+ class.

The reverse side of the sheet is painted with a two-layer grey backside coating.

GreenCoat Pro BT complies with current REACH regulations and is fully free of chromates.

SSAB’s color coated steels are all manufactured according to EN 10169.

SSAB Zero™ and GreenCoat are trademarks of the SSAB group of companies.

Technical Properties

Technical Properties
Technical Properties
Gloss
Regular
40
Matt
10
Technical Properties
Technical Properties
Minimum inner bending radius
Regular
1.5 x sheet thickness
Matt
1.5 x sheet thickness
Technical Properties
Technical Properties
Scratch resistance
Regular
35 N
Matt
35 N
Technical Properties
Technical Properties
Lowest forming temperature
Regular
-15 °C
Matt
-15 °C
Technical Properties
Technical Properties
UV radiation resistance
Regular
RUV3
Matt
RUV3
Technical Properties
Technical Properties
Corrosion resistance 1)
Regular
RC5
Matt
RC5
Technical Properties
Technical Properties
Stain resistance
Regular
Very good
Matt
Very good
Technical Properties
Technical Properties
Highest operating temperature
Regular
100 °C
Matt
100 °C
Technical Properties
Technical Properties
Fire classification, EN 13501-1
Regular
A2 s1 d0
Matt
A2 s1 d0
Technical Properties
Technical Properties
Coating thickness, nominal (primer + top coat)
Regular
36 µm
Matt
36 µm
Technical Properties
Technical Properties
Coating structure
Regular
Structured
Matt
Structured
Technical Properties
Technical Properties
Steel designation 2)
Regular
S280GD Zero, S350GD Zero*, DX51D Zero*
Matt
S280GD Zero, S350GD Zero*, DX51D Zero*
Technical Properties
Technical Properties
Zinc coating
Regular
275 g/m2
Matt
275 g/m2
Technical Properties
Technical Properties
Min steel thickness 2)
Regular
0.50 mm
Matt
0.50 mm
Technical Properties
Technical Properties
Steel width 2)
Regular
1000 - 1500 mm
Matt
1000 - 1500 mm
* Trial deliveries

1) Classification into corrosion resistance categories is based on blistering, delamination and damage on bend of the coating after two years exposure in natural outdoor testing sites as specified in EN 10169.

2) Maximum steel thickness for S280GD Zero is 0.75 mm. Maximum steel width depends on steel thickness. For other steel dimensions or steel grades please contact SSAB Tech Support.

Colors

Below are the colors currently available. Other colors can be agreed upon separately.

Colors shown in the color table are only indicative. To see the real visual appearance of the product, please order a color sample. Please note also that the same colors between the products may differ.

For information on thermal properties (solar reflectance index SRI or thermal emittance TE) of available colors, please contact SSAB Tech Support.

Note for Metallic colors: To ensure tonal consistency of colors on a single exterior face, all material must come from the same production batch. Also the directionality of surfaces has to be consistent especially when sheets are cut to size.

Reverse Side Coating

Unless otherwise specified, the reverse side of the sheet is painted with a two-layer coating to further improve the corrosion resistance of the end product. The coating provides good adhesion properties to many adhesives and foams; nevertheless the compatibility needs to be tested case-specifically.

Technical Properties
Technical Properties
Nominal Coating Thickness (primer + top coat)
12 µm
Technical Properties
Technical Properties
Color
Grey
Technical Properties
Technical Properties
Corrosion Resistance
Min CPI3

For easy material identification the reverse side of the sheet is stamped with the GreenCoat logo and the product name. The production date is marked to ease material traceability and can be referred to within the guarantee period. An arrow shows the direction of production to ensure installation in a uniform direction.