Download data sheet

General Product Description

Hardenable boron steel for the automotive industry. Docol PHS 2000 steels are optimized for parts and components that are manufactured by direct or indirect hot stamping. Applications include safety parts such as bumper systems, door impact beams, and B-pillar reinforcements.

Dimension Range

Cold rolled / UC: thickness 1.00-2.10 mm, width up to 1515 mm.

Hot rolled / UC*: thickness 2.00-4.00 mm, width up to 1600 mm.

Slit strip and cut to length sheets are available upon request.

*Available upon request.

Mechanical Properties

Docol PHS FH 2000

Standard
SSAB
Condition
Full Hard
Test direction
T
Typical yield strength Rp0.2 (MPa)
980
Typical tensile strength Rm (MPa)
1100
Typical elongation A80
(%)
4
Typical elongation A5
(%)
—

Docol PHS CR 2000

Docol PHS HR 2000+A

Standard
SSAB
Condition
Annealed
Test direction
T
Typical yield strength Rp0.2 (MPa)
330 2)
Typical tensile strength Rm (MPa)
540
Typical elongation A80
(%)
27
Typical elongation A5
(%)
31

1) Properties depend on the process.

2) ReH is used instead of Rp0.2.

Chemical Composition (ladle analysis)

C
(%)
C
(%)
0.30 - 0.38
Si
(%)
0.15 - 0.35
Mn
(%)
1.10 - 1.50
P
(max %)
0.025
S
(max %)
0.005
Cr
(max %)
0.35
B
(%)
0.0010 - 0.0050
Nb+Ti
(max %)
0.2

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Hot rolled (UC): Tolerances in accordance to EN 10051.

Customized dimensional and shape tolerances are available upon request.

Surface Treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® PHS steel product offer

Docol® PHS 1500 press hardening

제품 보기

Docol® PHS 1800 press hardening

제품 보기

Docol® PHS 2000 press hardening

제품 보기

관련 내용

시험용 재료 재고

자동차에서 독창적인 적용분야를 발견하거나 새로운 생산 방식을 시도해 보길 원하십니까, 또는 연비와 내충돌성, 지속가능성을 향상시키기 위해 부품을 더욱 가볍게 제작하길 원하십니까?

자세히 알아보기

Docol® AHSS 강재 성형 데이터

기존의 Docol® 고객들은 자동차용 고장력강 선택과 시뮬레이션에 필요한 성형 데이터에 언제든지 접근할 수 있습니다.

자세히 알아보기