Customer story

Al Jeathen reduces tipper weight while increasing payload capacity with Hardox® 500 Tuf steel

Customer story, SSAB World
February 29, 2024 8:22 CET
Since making Hardox® 500 Tuf steel its material of choice, leading Saudi Arabian heavy-transport equipment manufacturer Al Jeathen has seen its products last longer, weigh less and become more sustainable.

Al Jeathen was founded in 1983 in Riyadh, the capital of Saudi Arabia, and is now one of the country’s largest manufacturers of heavy-transport equipment. It produces all types of water and fuel tankers as well as trailers and semi trailers.

Since 2022, Al Jeathen’s trailer bodies are made entirely in Hardox® 500 Tuf steel after upgrading from Hardox® 450. So why the switch?

“Our products are quite heavy, so we were looking at solutions that could bring the trailer weight down and payload capacity up on each trip by the equivalent amount. Hardox 500 Tuf provided that,” says Ali Al Jeathen, General Manager at Al Jeathen in Al-Kharj.

Why less means more

Hardox® 500 Tuf is perfect for designing weight-optimized trailer bodies. In Al Jeathen’s case, their 22 cubic meter trailer bodies were earlier built with 6mm and 8mm mild steel. Today they are built with Hardox® 500 Tuf 4mm. As a result, the tipper body now weighs less than 2 tons – which is 2,5 tonnes less than before.

“By upgrading to Hardox 500 Tuf steel, we’ve been able to reduce the weight of our 22 cubic meter trailers by around 20 percent compared to Hardox 450, thus increasing the load capacity by the same number of kilograms,” says Ali Al Jeathen.

Reducing the weight and thickness of the steel is just one option when upgrading from Hardox® 450 to Hardox® 500 Tuf, according to Mohammed Khatib, SSAB’s Regional Sales Manager. The other option is to keep the same thickness and instead increase the lifetime of the steel by 40 percent.

“One of the biggest benefits when upgrading from Hardox 450 to Hardox 500 Tuf is that you get a more high-end product without changing any tools or processes in the workshop,” says Mohammed Khatib.

“The partnership with SSAB has been a success for us. They always support us in terms of technical aspects and always help us to find solutions to existing problems until they are solved.”

Ali Al Jeathen, General Manager at Al Jeathen

More than a supplier

Al Jeathen describes SSAB as a good and important partner that gives Al Jeathen dedicated technical support on material selection, bending, welding as well as optimizing its production.

“The partnership with SSAB has been a success for us. They always support us in terms of technical aspects and always help us to find solutions to existing problems until they are solved,” says Ali Al Jeathen.

Member of the Hardox® In My Body program

Al Jeathen has been a SSAB customer since it began using Hardox® steel in 2019 and since February 2022, it has also been a member of the Hardox® In My Body customer program.

“The certification proves that our products have been manufactured according to the highest quality standards,” says Ali Al Jeathen.

In addition, as a result of the Hardox® In My Body program, the company’s geographic reach and catchment area has also been expanded.

About Al Jeathen


 

www.aljeathen.com

1/8

Contact us

No matter where you are located, we have local support that can answer your questions.

Sign up for our newsletters

Sign up for our newsletters and manage your subscriptions

Take advantage of the benefits now

Hardox banner

Hardox® wear plate

Hardox® wear plate is the world’s leading abrasion-resistant (AR) steel. Hardox® is hard through and through, from surface to core, giving you an extended service life and high productivity in even the toughest environments.

tipper

Hardox® in My Body

Look for the Hardox® in My Body mark when you're looking for products that are hard, tough, cost-effective and made of genuine Hardox® wear plate.

Related articles

Customer storyNTT Group extends product service life by upgrading to Hardox® HiAce steel
Customer story, SSAB World
Customer storyHow CTE maximized the performance of its truck-mounted lifting platforms with Strenx® performance steel
Customer story, SSAB World
Customer storyHow PT Sanggar Sarana Baja increased payload capacity with Hardox® wear plates
Customer story, SSAB World