Move cargo – not steel

1 min read

""

Product

Country

Company

Industry

Trailers and body builders

By removing stiffeners and using the high load and lifetime performance of Hardox® 450, the weight could be reduced by 35% at the same time as the lifetime doubled from 6 years to 12 years.

SSAB EcoUpgraded

Together with our customers, SSAB continually upgrades steel and equipment designs. SSAB EcoUpgraded saves CO2 both in steel production and during the full lifetime of the machine.

From the CO2 payback time and onwards, every extra hour brings additional savings.

EcoUpgraded logo

Savings on CO₂

SSAB EcoUpgraded Scrap recycling container
Calculation data
Fuel consumption, fully loaded34 litres/100 km
Fuel consumption, without load24 litres/100 km
Machine usage per year100 000 km/year
Distance with maximum load50 %
Service lifetime12 years
Maximum payload (before upgrading)13 260 kg
Gross weight (fully loaded)26 000 kg
Weight of original parts4 020 kg
Weight of upgraded parts2 620 kg
Wear resistance stee saved during lifetime4 202 kg