SSAB Opti™ Cut is structural quality steel specifically designed to enhance laser cutting performance. SSAB Opti™ Cut meets and exceeds the requirements of the relevant ASTM and Canadian Standards Association (CSA) specifications. Dual and multiple certifications to ASTM A36, A572-50, A656-50 and CSA G40.21 38W, 44W and 50W specifications are avaiable upon request.
1) Standard thicknesses 5/8 in., 3/4", 1.0 in., 1.25 in., and 1.50 in. Please inquire for non-standard thicknesses.
2) Standard thicknesses 1-3/4" and 2 in. Please inquire for non-standard thicknesses.
3) Standard widths 60 in., 72 in., 96 in., and 120 in. Please inquire for non-standard widths.
4) Standard lengths 240 in. and 480 in. Please inquire for non-standard lengths.
Tensile Properties: Tensile testing is performed in the transverse direction according to ASTM A6 requirements.
1) Single value represents minimum tensile strength requirement.
2) Elongation requirements for plates wider than 24 in.
Charpy V-notch impact testing performed with longitudinal specimens in accordance with ASTM 673, H frequency.
1) For each reduction of 0.01 percentage point below 0.25% C, an increase of 0.06 percentage point manganese above 1.20% is permitted up to a maximum of 1.35%.
2) Carbon Equivalent (CE) = C +Mn/6 + (Cr+Mo+V)/5 + (Cu+Ni)/15
SSAB Opti™ Cut cut-to-length plates are produced to 1/2 of the ASTM A6 permitted variation over the specified thickness and to the restrictive plate flatness requirements of ASTM A6. Width and length tolerances for SSAB Opti™ Cut are in accordance with ASTM A6.