SSAB Opti™ Cut CTL

Download data sheet

General Product Description

SSAB Opti™ Cut is structural quality steel specifically designed to enhance laser cutting performance. SSAB Opti™ Cut meets and exceeds the requirements of the relevant ASTM and Canadian Standards Association (CSA) specifications. Dual and multiple certifications to ASTM A36, A572-50, A656-50 and CSA G40.21 38W, 44W and 50W specifications are avaiable upon request.

Available Dimensions

Product type
Product type
Hot-Rolled, Cut-to-Length Plate 1)
Thickness 2)
(inmm)
0.188 - 0.5004.78 - 12.7
Width 3)
(inmm)
60 - 961500 - 2400
Length 4)
(inmm)
120 - 2403050 - 6100

1) Temper-leveled plate. SSAB's Cut-to-Length facilities use the temper leveled coil (TLC) process to produce temper-leveled plate For additional infomration concerning our temper-leveling process, please refer to our SSAB Americas: North American Cut-to-Length Operations brouchure located under the Downloads section of our Commercial Steels Overview webpage.

2) Standard thickness 3/16 in., 1/4 in., 3/8 in., and 1/2 in. Please inquire for non-standard thickness.

3) Standard widths 60 in., 72 in., 96 in. Please inquire for non-standard widths.

4) Standard lengths 120 in. and 240 in. Please inquire for non-standard lengths.

Mechanical Properties

Tensile Properties:  Tensile testing is performed in the transverse direction according to ASTM A6 requirements.

Thickness
(inmm)
Thickness
(inmm)
0.188 - 0.5004.78 - 12.7
Yield strength
(min ksi)
50
Tensile strength
(ksi)
65 - 80
Elongation in 2" 1)
(min %)
21
Min. inner bending radius for a 90° bend 2)
(x t)
1

1) Subject to Elongation Requirement Adjustments of ASTM A6 for thickness less than 0.312 in.

2) Minimum inside bending radius guarantee for both longitudinal and transverse bending orientations.

Impact Properties

Grade
Grade
SSAB OptiTM Cut
Min. impact energy for longitudinal testing,
Charpy V 0.393x0.393" test specimen 1)
40 ft-lbs / -22 °F

Charpy V-notch impact testing performed with longitudinal specimens in accordance with ASTM 673, P frequency.

1) Absorbed energy values obtained for subsize specimens shall not be less than the applicable values of ASTM A370, Table 10 which are proportional to the absorbed energy values required for full-size specimens.

Chemical Composition

Thickness (inmm)
Thickness (inmm)
0.188 - 0.5004.78 - 12.7
C
(max wt %)
0.10
Mn
(wt %)
0.80 - 1.20
P
(max wt %)
0.02
S
(max wt %)
0.006
Si
(max wt %)
0.05
CE 1)
(max wt %)
0.30

1) Carbon Equivalent (CE) = C +Mn/6 + (Cr+Mo+V)/5 + (Cu+Ni)/15

Tolerances

SSAB Opti™ Cut cut-to-length plates are produced to 1/2 of the ASTM A6 permitted variation over the specified thickness and to the restrictive plate flatness requirements of ASTM A6.  Width and length tolerances for SSAB Opti™ Cut are in accordance with ASTM A6.

Fabrication and Other Recommendations

SSAB Opti™ Cut plates have been optimized for laser cutting, cold forming and welding. For information concerning fabrication, see SSAB's brochures on www.ssab.com or consult Tech Support. Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products. Contact information www.ssab.com