Docol® 1700M martensitic

Download data sheet

General Product Description

A martensitic steel for automotive applications, Docol 1700M allows for increased crashworthiness, lightweight design and cost-efficient production methods for the automotive industry. Docol 1700M is one of the strongest cold rolled advanced high-strength steels on the market and has become the material of choice for automotive applications such as bumper systems and structural components.

Dimension Range

Cold rolled / UC: thickness 1.00-2.10 mm, width up to 1250 mm.

Mechanical Properties

Docol CR1350Y1700T MS

Standard
VDA 239-100
Coating
UC
Test direction
L
Yield strength Rp0.2
(MPa)
1350 - 1700
Tensile strength Rm
(MPa)
1700 - 2000
Elongation A80
(min %)
3
BH2
(min MPa)
30
Min. inner bending radius for a 90° bend
4.0 x t

Chemical Composition (ladle analysis)

Docol CR1350Y1700T MS

Coating
UC
C
(max %)
0.35
Si
(max %)
1.00
Mn
(max %)
3.00
P
(max %)
0.020
S
(max %)
0.010
Al
(%)
From 0.010
Nb+Ti
(max %)
0.15
Cr+Mo
(max %)
1.00
B
(max %)
0.010
Cu
(max %)
0.20

Tolerances

Cold rolled (UC): Tolerances in accordance to EN 10131.

Customized dimensional and shape tolerances are available upon request.

The following improved flatness tolerances are available for cold rolled martensitic products upon request. The tolerances are valid for mother coils only before slitting.

Thickness
(mm)
Thickness
(mm)
1.00 - 1.39
Max height 1)
(mm)
8
Thickness
(mm)
Thickness
(mm)
1.40 - 1.59
Max height 1)
(mm)
7
Thickness
(mm)
Thickness
(mm)
1.60 - 1.79
Max height 1)
(mm)
6
Thickness
(mm)
Thickness
(mm)
1.80 - 2.10
Max height 1)
(mm)
5

1) Distance from the top surface of the strip normal to flat surface. Measured with a ruler on sheets of mother coil width and minimum length 1200 mm. Cross bow and coil set excluded.

Surface treatments

Uncoated (UC): available as oiled.

All surface treatments are in accordance with RoHS directive (2011/65/EU) and do not contain Chromium VI (Cr6+). Surface treatments provide only temporary surface protection during transportation and storage. In order to avoid corrosion damages, care must be taken to keep the products dry during transportation and storage. If they become wet, they must be separated and situated so that they are dried quickly.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® Martensitic steel product offer

Docol® 900M martensitic

View product

Docol® 1100M martensitic

View product

Docol® 1200M martensitic

View product

Docol® 1300M martensitic

View product

Docol® 1400M martensitic

View product

Docol® 1500M martensitic

View product

Docol® 1700M martensitic

View product

Related content

AHSS trial material stock

Want to discover unique automotive applications for AHSS materials? Try new production methods? Or create lighter components that can improve fuel efficiency, crash-worthiness and sustainability?

Read more

Automotive steel applications

Docol® steel grades serve specific design purposes and are chosen by designers for a wide range of applications and used by OEMs and tier suppliers in millions of vehicles around the world.

Read more

Forming data for Docol® AHSS steels

Existing Docol® customers get 24/7 access to the forming data you need to help in your selection and simulation of automotive advanced high strength steels.

Read more
Copyright 2026