Docol® 420HE high edge ductility

Download data sheet

General Product Description

The Docol HR420Y480T HE steel is the next generation of hot-rolled high-strength low-alloy steels with improved local formability for higher edge ductility and cut-edge quality.

Docol HR420Y480T HE have a new and closely controlled production method resulting in a very fine microstructure in combination with a very clean steel, resulting in greatly improved local formability while still retaining a good global formability making it suitable for stamping most geometries and will excel in demanding forming where the cut edges may limit the forming operation.

The improved cut edge quality achieved with this new way of producing Docol HR420Y480T HE with a steel less sensitive to tool-settings and –wear compared to conventional HSLA grades, make it especially suitable for fine blanking.

Combining the improved local formability with the excellent cut-edge quality Docol HR420Y480T HE will have a typical hole expansion of approx. 30 percentage points above the corresponding conventional HSLA grade.

Also the bending performance is improved and a bend radius of 0xt can be guaranteed.

Docol HR420Y480T HE will excel when optimizing any fine blanking, stamping or forming operation and will push the limit on how to utilize the benefits of steel.

Docol HR420Y480T HE can after agreement be adapted and delivered as dual certified with S420MC according to EN 10149-2.

Dimension Range

Docol HR420Y480T HE is available as Hot-rolled pickled and oiled coil, slit coils and cut to length sheets in thickness of 2.00*) - 7.00 mm and widths up to 1600 mm. Length up to 16 meters.

*)Some restrictions may occur, and will be handled on request.

Mechanical Properties

Docol HR420Y480T HE

Coating
UC
Yield strength Rp0.2
(min MPa)
420
Tensile strength Rm
(MPa)
480 - 600
Elongation A80 1)
(min %)
18
Elongation A5 2)
(min %)
22
Hole expansion ratio 3)
(% typical)
90
Min. inner bending radius for a 90° bend
0.0 x t

The mechanical properties are valid in the longitudinal direction.

Bending properties for both longitudinal and transversal direction.

1) A80 value applies for thicknesses < 3.00 mm.

2) A5 value applies for thicknesses ≥ 3.00 mm.

3) HER –ratio is average of three test results out of five tested samples by excluding minimum and maximum results.

Chemical Composition (ladle analysis)

Docol HR420Y480T HE

C
(max %)
0.10
Si
(max %)
0.03 1)
Mn
(max %)
1.50
P
(max %)
0.025
S
(max %)
0.010
Altot
(min %)
0.015
Nb
(max %)
0.09 2)
V
(max %)
0.20 2)
Ti
(max %)
0.15 2)

The steel is grain refined.

1) Meets the requirements of category A (thin coatings) for hot-dip zinc-coating in EN 10149-2.

2) The sum of Nb, V and Ti is max 0.22%.

Tolerances

Hot-rolled (UC): Tolerances in accordance to EN 10051.

Customized dimensional and shape tolerances are available on request.

Fabrication and Other Recommendations

For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.

Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.

Docol® High Edge Ductility steel product offer

Docol® 355HE high edge ductility

View product

Docol® 420HE high edge ductility

View product

Docol® 460HE high edge ductility

View product

Docol® 500HE high edge ductility

View product

Docol® 550HE high edge ductility

View product

Related content

AHSS trial material stock

Want to discover unique automotive applications for AHSS materials? Try new production methods? Or create lighter components that can improve fuel efficiency, crash-worthiness and sustainability?

Read more

Automotive steel applications

Docol® steel grades serve specific design purposes and are chosen by designers for a wide range of applications and used by OEMs and tier suppliers in millions of vehicles around the world.

Read more

Forming data for Docol® AHSS steels

Existing Docol® customers get 24/7 access to the forming data you need to help in your selection and simulation of automotive advanced high strength steels.

Read more
Copyright 2026