    General Product Description

    Lloyd’s Register Grade AH27S is a higher-strength structural steel with a specified minimum yield strength of 38.5 ksi and specified minimum Charpy V-notch impact toughness properties.

    Applications

    Typical applications include ships and other structural applications.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (inchesmm)
      Width
      (inchesmm)
      Length
      (inchesmm)
      Grade AH27S Plate 0.1875 - 1.504.762 - 38.1 72 - 1201800 - 3050 240 - 10206100 - 25910
      Compare parameters

      Select one parameter to compare

      Comparison

        Width: Please inquire for plate widths less than 72 in. and inquire plate product over 120 in.

        Length: Please inquire for plate lengths outside the noted ranges.

        Thickness: Please inquire for plate thicknesses outside the noted ranges.

        Mechanical Properties

        Tensile testing is performed in the transverse direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Product type Thickness
          (inchesmm)
          Yield strength
          (min ksi)
          Tensile strength
          (ksi)
          Elongation A5 1)
          (min %)
          Grade AH27S Plate 0.1875 - 1.504.762 - 38.1 38.5 58 - 77 22
          Compare parameters

          Select one parameter to compare

          Comparison

            1) See Lloyd’s Register Rules for elongation requirements for alternative tensile specimens.

            Impact Properties

            Hide/Show specific columns Edit
            Select columns to display
              Grade Thickness
              (inchesmm)
              Test temperature
              (°F)
              Min Longitudinal Average Energy 1)
              (ft-lbs)
              Min transverse average energy 1)
              (ft-lbs)
              Grade AH27S 0.1875 - 1.504.762 - 38.1 32 20 15
              Compare parameters

              Select one parameter to compare

              Comparison

                1) Tests are to be taken in the longitudinal direction. Normally, transverse test specimens are not required unless otherwise specified in the order. Generally, impact tests are not required when material thickness is less than 0.236 in.

                No more than one value below the specified minimum average energy but no less than 70% of the specified minimum average energy value.

                Minimum average energy for full-size specimens. Refer to Lloyd’s Register Rules for sub-size specimen energy requirements.

                Carbon Equivalent CET(CEV)

                Hide/Show specific columns Edit
                Select columns to display
                  Grade Grade AH27S
                  Thickness (inchesmm) 0.1875 - 1.504.762 - 38.1
                  CEV 1) (max %) 0.36
                  Compare parameters

                  Select one parameter to compare

                  Comparison

                    Grade
                    Thickness (inchesmm)
                    Grade AH27S
                    0.1875 - 1.504.762 - 38.1
                    Grade
                    CEV 1) (max %)
                    Grade AH27S
                    0.36

                    1) Carbon equivalent requirements for TMCP condition of supply only.