ASTM A387 Gade 12

Download data sheet

General Product Description

The ASTM A387 specification is the Standard Specification for Pressure Vessel Plates, Alloy Steel, Chromium-Molybdenum intended primarily for use in welded boilers and pressure vessels designed for elevated temperature service. The two grades SSAB produces are available as Class 1 and/or Class 2.

Dimension Range

Grade
Grade
Grade 12
Product type
Plate
Thickness
(inmm)
0.276 - 2.007.01 - 50.8
Width
(inmm)
75 - 129.91900 - 3299
Length
(inmm)
154 - 5903910 - 15000

Width: Inquire for widths and lengths outside the noted ranges.

Mechanical Properties

Product type
Product type
Plate
Grade
Grade 12 Class 1
Thickness
(inmm)
0.276 - 2.007.01 - 50.8
0.2% YS
(ksi)
33
UTS
(ksi)
55 - 80
Elongation in 2" 1)
(min %)
22
Elongation in 8" 1)
(min %)
18
Product type
Product type
Plate
Grade
Grade 12 Class 2
Thickness
(inmm)
0.276 - 2.007.01 - 50.8
0.2% YS
(ksi)
40
UTS
(ksi)
65 - 85
Elongation in 2" 1)
(min %)
22
Elongation in 8" 1)
(min %)
19

1) Refer to ASTM A20/A20M for Elongation adjustments based on plate thickness.

Show specs in: