Hardox® HiAce doubles service life of reclaimer buckets

Hardox, Hardox HiAce
September 26, 2024 11:07 CEST
Mining operations demand tough equipment that can withstand extreme impacts, stresses and wear, day in and day out. Compromising on quality — and safety — can be costly, and keeping operating costs under control is a non-negotiable. You’ve got to build your machinery with the best steels possible to not only stand up to the job, but to boost long-term productivity.

This is where Hardox®HiAce wear steel comes into play as a significant factor. Mining and processing copper ore creates corrosive agents such as sulfuric acid and iron sulfates, which attack steel and decrease the service life of equipment used for excavating and transporting the ore.

A case in point is the reclaimer buckets for wheel excavators operated by one of the largest copper producers in the world. This company was not satisfied with the service life of their buckets and asked one of SSAB’s steel service centers to come up with a better solution.

Enter Hardox®HiAce

Hardox® HiAce is a recent steel grade developed by SSAB with the sole purpose of resisting corrosive wear. This wear steel has a nominal hardness of 450 HBW, the same as the well-established grade Hardox® 450. Under non-corrosive wear conditions, they both provide the same high service life. The distinction lies in how the steels perform when exposed to acidic low pH environments.

If corrosion is present, Hardox® HiAce can increase service life by 2 to 3 times compared to a 450 HBW steel, depending on the abrasive materials and the acidic conditions.

This made Hardox® HiAce a natural choice when the company wanted to design and manufacture new reclaimer buckets. Hardox® HiAce was used for the bucket’s floor and sides, which are exposed to corrosive materials.

Based on the mining conditions these buckets are operating in, the company expects to get twice the service life compared to its previous buckets.

The mechanics of corrosive wear

Corrosive wear is caused by oxidation of the steel’s surface. The oxidation process reduces the hardness of the surface, resulting in an accelerated wear rate. This leads to higher repair costs and a shorter service life than expected – which, of course, can negatively impact productivity and profitability.

Hardox® HiAce properties

A selection of Hardox® HiAce specifications:

Typical impact toughness 50 J at -40°C (37 ft lbat -40°F).

Thickness range 3 to 100 millimeters (0.118" to 3.937").

Excellent workshop properties.

Get the advice you need by contacting us, and speak directly with our technical specialists.

En bild som visar hjul, himmel, utomhus, fordon

Automatiskt genererad beskrivning

Reclaimer buckets made in Hardox®HiAce for wheel excavator.

En bild som visar mark, Fordonsdelar, tåg, utomhus

Automatiskt genererad beskrivning

When changing to Hardox® HiAce in the reclaimer buckets, SSAB’s customer expects them to last twice as long as the previous buckets.

En bild som visar byggnad, hjul, utomhus, ask

Automatiskt genererad beskrivning

To resist the acidic conditions from the copper ore, the buckets’ floor and sides are made with Hardox® HiAce.

En bild som visar himmel, utomhus, solnedgång, bro

Automatiskt genererad beskrivning

Reclaimer buckets at one of Chile’s largest copper mines.

Related articles

Apr 10Product press releases
Hardox
Hardox HiAce

Corrosive environments in combination with wear, can wreak havoc on heavy equipment. Even materials or aggregates that aren’t usually aggressive can cause corrosion under the right conditions. While...

Sep 11Product press releases
Hardox
Hardox HiAce

Hauling ore in hot and humid climates can have a devastating effect on the abrasion resistance of conventional abrasion-resistant steels. Bruce Rock Engineering in Australia was familiar with the...

Apr 8Product press releases
Hardox

Don’t let looks deceive you. Building a bucket entirely with Hardox® 500 Tuf wear plate results in enhanced wear performance, less need for maintenance and less fuel consumption due to reduced bucket...