This off-highway hauler is fit for multiple purposes; it can haul material, carry a water tank or be a flexible service module. The truck is designed to be fitted with different modules depending on the need. A clever redesign of the high strength steel chassis reduced the weight of the chassis by 27%, increasing the load capacity and reducing fuel consumption.
Together with our customers, SSAB continually upgrades steel and equipment designs. SSAB EcoUpgraded saves CO2 both in steel production and during the full lifetime of the machine.
From the CO2 payback time and onwards, every extra hour brings additional savings.


| Calculation data | |
| Fuel consumption, fully loaded | 36 litres/100 km |
| Fuel consumption,without load | 20 litres/100 km |
| Machine usage per year | 5 000 km/year |
| Distance with maximum load | 50 % |
| Service lifetime | 8 years |
| Maximum payload (before upgrading) | 60 000 kg |
| Gross weight (fully loaded) | 98 000 kg |
| Weight of original parts | 4 400 kg |
| Weight of upgraded parts | 3 200 kg |