Slurry pipelines, stone quarry tubes and pipes in Hardox® wear plate

If you want to increase the lifetime of slurry pipelines, tubes used in stone quarries and other pipes subject to wear and abrasion, you’ve got many good reasons to try out Hardox® tubes.

Field tests have proved that Hardox® Tube 400 and Hardox® Tube 500, with a hardness grade of 400 HB and 500 HB, last 2.5 and 4 times longer, respectively, than mild steel when pumping wet concrete. Hardox® tubes were also successfully introduced in pneumatic powder conveying systems for clinker and glass. They also deliver superior wear resistance in other mining machinery and equipment.
A screening bucket in a harsh environment made by Remu

Hard-working screening buckets rely on Hardox® tubes

Remu Oy has been using Hardox® steel for a long time and knows that this wear-resistant material is second to none. The proof is in the high productivity and long-lasting performance of its products.

Read the full story
WearCalc calculator app or desktop version for calculating equipment wear and service life.

WearCalc – Maximize equipment wear resistance and calculate the savings

WearCalc™ 3.2.5 makes tough decisions about choosing the right wear plate easy.

Read more

Hardox® wear plate, the unrivaled choice for extreme wear challenges

Hardox® wear plate is the leading abrasion-resistant (AR) steel. Hard through and through, from the surface deep down to its core. Delivering extended service life and high productivity, it exceeds expectations in the most challenging, extreme wear environments. Why settle for anything else?

Read more