Curran Contracting Stokes Asphalt Production with Hardox® wear plate

3 min read

Country

United States

Company

Curran Contracting

Industry

Construction, demolition & road building machinery

Curran Contracting’s Hardox® wear plate asphalt dryer flights save estimated $10K in labor costs. Watch how James Cassem the Asset Director at Curran Contracting ramps up efficiency, seizes savings and stokes the company’s material production by upgrading asphalt dryer wear parts to Hardox® wear plate.

Curran Contracting is known for high-performance infrastructure work — mass excavation, site development, asphalt paving, and road construction. With three high-capacity asphalt production plants in Illinois and more than 1,200 pieces of yellow iron running daily, uptime is everything. Their goal is simple: keep material moving, keep plants producing, and avoid costly interruptions.

“Our high-capacity plants run the newest, state-of-the-art equipment and mixers to meet project requirements,” explains Cassem. “We’re continually adding new and innovative products to our processes and operations to meet our customers’ demands for high quality.”

Watch the whole story

Watch the full story in the video

See how Curran Contracting partnered with certified Hardox® Wearparts center Ecco Fab to save on labor costs and increase operational efficiency.

“We ran 250,000 tons across them and had no wear at all,” says Cassem. “We estimate a $10,000 per year in labor savings alone, and that’s not including the reductions in downtime or cost of emergency maintenance repairs.”

Where extreme heat and nonstop production meet

With an eye on continuous improvement, Cassem spotted a production bottleneck within the asphalt production process that frequently halted operations, bringing costly labor for repairs and expensive downtime.

The problem centered around the asphalt dryer, which must withstand not only the abrasive aggregate moving through the drum at 300 to 450 tons per hour, but also intense heat with shell temperatures reaching up to 650°F (343.33°C). Inside the drum, the flights (also known as “buckets”) lift and cascade the aggregate to ensure even drying. These components face relentless heat, abrasion, and impact.

Explore Hardox® wear plate for high temperatures

Trust the experts certified for solutions and wear parts built to last

“Hardox® is the Cadillac of steel. It can take a lot of abuse,” Bauer says. ”Through our 40 years of experience with Hardox® products, we have developed industry-leading techniques in collaboration with end-users. Every part is custom-made according to my client’s specifications in our production facility, centrally located in Rockford, Illinois.” 

Bauer recognized how the original material was not formulated specifically for environments with excessive heat and abrasion.

To illustrate the difference, Bauer compared two identical dryer cups side by side:

  • Factory cup: After six years, worn nearly thin, edges rounded, material almost gone.
  • Hardox® wear plate cup: Six years, same tonnage, same run time — and it looked virtually new. Sharp corners. Minimal wear. Higher durability.
Why settle for less in your wear parts?

Not all abrasion resistant steels are created equal

According to Bauer, the material is designed for temperatures up to 950°F, far beyond the 375°F threshold of standard AR steel, and even if it turns cherry-red, Hardox® maintains performance. Curran installed the first Hardox® wear plate flights and monitored performance closely. 

Immediate impacts from the initial upgrade:

  • No flight replacements needed for a year
  • Significant reduction in repair labor hours
  • Increased uptime for the high-capacity asphalt plant
  • Consistent heat resistance in the drum’s harshest areas

Curran began with five units. Now they’re operating 60 Hardox® wear plate flights across their operation. The improved durability and reliability give Curran a measurable competitive advantage in a demanding, nonstop industry.

Cassem concludes, “Nothing has shown as much benefit as the Hardox® product we’re using. No regrets at all. I’d make that decision a thousand times over.”

Explore the full Hardox® wear plate portfolio

Ready to step up your steel?

Join companies like Curran Contracting and step up from average abrasion-resistant (AR) steel to Hardox® wear plate, the world’s only resistant steel hard and tough for extreme applications. Ask us how to get your hands on a sample.

I’m ready to step up my steel

Stay up to date on the benefits of Hardox® wear steel

Survival of the fittest

In nature, only the best-adapted survive. In the world of steel, it’s no different. When equipment faces extreme wear, only the hardest and toughest materials endure. Where others fail, Hardox® wear plate keeps performing.

See how
A hand holding the mobile app Hardox® Wearcalc, which calculates wear for different Hardox® steel grades

Find the right type of wear plate

Try our Hardox® WearCalc application and calculate how long the life of your products will increase and the payload will increase with a replacement for a Hardox® wear plate.

Download the WearCalc application
Black and white logo of Hardox® In My Body on a tipper body.

Guarantee of a good choice

The Hardox® In My Body brand on your devices is a guarantee of quality, performance and reliability.

Introduction to the Hardox® In My Body brand