Less weight makes light work
December 20, 2019 6 min read
![""](/-/media/images/customer-cases/ecoupgraded/new-layout-images/1920x570-ecoupgraded-cc-mining-backhoe-bucket-top-image.jpg?m=20210428105240)
Case details
The high productivity mining backhoe in Hardox® HiTuf, 450, 500 and 550 offers a totally new design concept, reducing the weight by up to 25% and increasing the payload capacity by up to 15%. This means fewer working cycles for the same load moved – in addition to additional safety and maintenance cost benefits.