Customer case
Winds of change – less drag, more load
October 30, 2018 6 min read
![""](/-/media/images/customer-cases/ecoupgraded/new-layout-images/1920x570-ecoupgraded-cc-roll-on-containers-top-image.jpg?m=20210428113939)
Case details
These containers were upgraded from 355 MPa standard steel to Hardox® 450, increasing the load capacity by 2,100 kg for the total vehicle with a set of three containers. This allows more payload per trip and also reduces the fuel consumption for the empty vehicle. The removal of stiffeners on the sides also lowers wind drag, which further reduces the fuel consumption.