ASTM A606 type 4

The ASTM A606 specification is the Standard Steel Specification for High-Strength, Low-Alloy, Hot Rolled and Cold Rolled Sheet and Strip Steel with Improved Atmospheric Corrosion Resistance for use in structural and other applications. A606 Type 4 steel has a minimum corrosion-resistance index of 6.0 based upon ASTM Guide G101.

Download data sheet

General Product Description

The ASTM A606 specification is the Standard Steel Specification for High-Strength, Low-Alloy, Hot Rolled and Cold Rolled Sheet and Strip Steel with Improved Atmospheric Corrosion Resistance for use in structural and other applications. A606 Type 4 steel has a minimum corrosion-resistance index of 6.0 based upon ASTM Guide G101.

Available Dimensions

Grade
Grade
Type 4
Product type
Coils
Thickness
(in)
0.079 - 0.394
Width
(in)
31.5 - 73

Product type: Inquire for Cut-to-Length product.

Thickness: Inquire for thicknesses outside the noted range.

 

Mechanical Properties

Tensile testing is performed in the longitudinal direction.

Product type
Product type
Coils
Thickness
(in)
0.079 - 0.394
Yield strength
(min ksi)
50
Tensile strength
(min ksi)
70
Elongation in 2"
(min %)
22