LR Grade 360 FG

Download data sheet

General Product Description

Lloyd’s Register Grade 360 FG is a killed, fine-grained carbon/carbon-manganese steel with a specified tensile strength range of 52 to 70 ksi.

Applications

Intended applications are for use in the construction of boilers and pressure vessels.

 

Available Dimensions

Grade
Grade
Grade 360 FG
Product type
Plate
Thickness
(in)
0.1875 - 1.50
Width
(in)
72 - 120
Length
(in)
240 - 1020

Width: Please inquire for plate widths less than 72 in. and inquire plate product over 120 in.

Length: Please inquire for plate lengths greater than the listed maximum.

 

Mechanical Properties

Tensile testing is performed in the transverse direction.

Grade
Grade
Grade 360 FG
Thickness
(in)
0.1875 - 0.630
Yield strength
(min ksi)
34
Tensile strength
(ksi)
52 - 70
Elongation A5 1)
(min %)
26
Grade
Grade
Grade 360 FG
Thickness
(in)
0.631 - 1.50
Yield strength
(min ksi)
31
Tensile strength
(ksi)
52 - 70
Elongation A5 1)
(min %)
26

1) See Lloyd’s Register Rules for elongation requirements for alternative tensile specimens.