    DNV Grades NV A36, NV D36, and NV E36 are high-strength structural steels with a minimum specified yield strength of 51 ksi and specified minimum Charpy V-notch impact toughness properties.

    Applications

    Typical applications include shipbuilding and mobile offshore drilling units and structures.

    Available Dimensions

    Hide/Show specific columns Edit
    Select columns to display
      Grade Product type Thickness
      (in)
      Width
      (in)
      Length
      (in)
      NV A36 Plate 0.1875 - 1.57 72 - 120 240 - 1020
      NV A36 Plate 1.58 - 2.00 72 - 120 240 - 600
      NV D36 Plate 0.1875 - 1.57 72 - 120 240 - 1020
      NV D36 Plate 1.58 - 2.00 72 - 120 240 - 600
      NV E36 Plate 0.1875 - 0.787 72 - 120 240 - 1020
      NV E36 Plate 0.79 - 2.00 72 - 120 240 - 600
      Compare parameters

      Select one parameter to compare

      Comparison

        Width: Please inquire for plate widths less than 72 in. and plate widths greater than 120 in.

        Length: Please inquire for plate lengths oustide the noted ranges.

        Thickness: Please inquire for plate thicknesses outside the noted ranges.

        Mechanical Properties

        Tensile testing is performed in the transverse direction.

        Hide/Show specific columns Edit
        Select columns to display
          Grade Thickness
          (in)
          Yield strength
          (min ksi)
          Tensile strength
          (ksi)
          Elongation A5 1)
          (min %)
          NV A36 0.1875 - 2.00 51 68 - 90 21
          NV D36 0.1875 - 2.00 51 68 - 90 21
          NV E36 0.1875 - 2.00 51 68 - 90 21
          Compare parameters

          Select one parameter to compare

          Comparison

            1) See DNV Rules for elongation requirements for alternative tensile specimens.

            Impact Properties

            Hide/Show specific columns Edit
            Select columns to display
              Grade Thickness
              (in)
              Test temperature
              (°F)
              Min Longitudinal Average Energy 1)
              (ft-lbs)
              NV A36 0.1875 - 2.00 32 25
              NV D36 0.1875 - 2.00 -4 25
              NV E36 0.1875 - 2.00 -40 25
              Compare parameters

              Select one parameter to compare

              Comparison

                1) Tests are to be taken in the longitudinal direction. Normally, transverse test specimens are not required unless otherwise specified in the order. Impact tests not required when material thickness is less than 0.236 in. unless otherwise specified.

                No more than one value below the specified miniminum average energy but no less than 70% of the specfied minimum average energy value.

                Minimum average energy for full-size specimens. Refer to DNV Rules for sub-size specimen energy requirements.

                Carbon Equivalent

                Hide/Show specific columns Edit
                Select columns to display
                  Grade NV A36 NV D36 NV E36
                  Thickness (in) 0.1875 - 2.00 0.1875 - 2.00 0.1875 - 2.00
                  CEV 1) (max wt %) 0.38 0.38 0.38